Final Magnetic Moment5.024 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.927 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.927 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRb + V |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 283.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 283.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 189.1 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 283.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 283.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 283.7 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 283.7 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 283.7 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 163.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 163.8 |
Al (mp-134) | <1 1 1> | <1 0 0> | 283.7 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 163.8 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 283.7 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 283.7 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 189.1 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 189.1 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 133.7 |
C (mp-48) | <0 0 1> | <1 1 1> | 163.8 |
NaCl (mp-22862) | <1 1 1> | <1 1 1> | 163.8 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 283.7 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 94.6 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 189.1 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 189.1 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 133.7 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 189.1 |
Ge (mp-32) | <1 1 1> | <1 0 0> | 283.7 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 189.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
52 | 51 | 51 | 0 | 0 | 0 |
51 | 52 | 51 | 0 | 0 | 0 |
51 | 51 | 52 | 0 | 0 | 0 |
0 | 0 | 0 | 2 | 0 | 0 |
0 | 0 | 0 | 0 | 2 | 0 |
0 | 0 | 0 | 0 | 0 | 2 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
1666.3 | -829.9 | -829.9 | 0 | 0 | 0 |
-829.9 | 1666.3 | -829.9 | 0 | 0 | 0 |
-829.9 | -829.9 | 1666.3 | 0 | 0 | 0 |
0 | 0 | 0 | 566.6 | 0 | 0 |
0 | 0 | 0 | 0 | 566.6 | 0 |
0 | 0 | 0 | 0 | 0 | 566.6 |
Shear Modulus GV1 GPa |
Bulk Modulus KV51 GPa |
Shear Modulus GR0 GPa |
Bulk Modulus KR51 GPa |
Shear Modulus GVRH1 GPa |
Bulk Modulus KVRH51 GPa |
Elastic Anisotropy8.31 |
Poisson's Ratio0.49 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TaZnOs2 (mp-979291) | 0.0000 | 0.013 | 3 |
Pm2HgGe (mp-863686) | 0.0000 | 0.000 | 3 |
NaMgTl2 (mp-865110) | 0.0000 | 0.000 | 3 |
Tm2CuRu (mp-865319) | 0.0000 | 0.000 | 3 |
TiNbTc2 (mp-865655) | 0.0000 | 0.000 | 3 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiGaFeCo (mp-998964) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoAs (mp-1066006) | 0.0000 | 0.211 | 4 |
MnGaFeCo (mp-999552) | 0.0000 | 0.044 | 4 |
Y3Sn (mp-1094256) | 0.0000 | 0.278 | 2 |
Sr3Yb (mp-981378) | 0.0000 | 0.041 | 2 |
Mg3Sb (mp-1094520) | 0.0000 | 0.205 | 2 |
Cr3Fe (mp-1008282) | 0.0000 | 0.171 | 2 |
Mg3Cd (mp-1038832) | 0.0000 | 0.056 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv V_pv |
Final Energy/Atom-2.0789 eV |
Corrected Energy-8.3155 eV
-8.3155 eV = -8.3155 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)