Final Magnetic Moment0.433 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.641 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.641 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRb + Ho |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 104.8 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 181.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 209.5 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 148.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 209.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 148.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 181.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 209.5 |
Al (mp-134) | <1 0 0> | <1 0 0> | 209.5 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 181.4 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 209.5 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 148.1 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 181.4 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 209.5 |
WSe2 (mp-1821) | <0 0 1> | <1 1 1> | 181.4 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 104.8 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 148.1 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 1> | 181.4 |
Au (mp-81) | <1 1 0> | <1 1 0> | 148.1 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 148.1 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 181.4 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 104.8 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 1> | 181.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2ZnCd (mp-984784) | 0.0000 | 0.007 | 3 |
AcYbGa2 (mp-979981) | 0.0000 | 0.000 | 3 |
PrHoZn2 (mp-976032) | 0.0000 | 0.010 | 3 |
Pr2AgRu (mp-861481) | 0.0000 | 0.033 | 3 |
Y2AgIr (mp-866160) | 0.0000 | 0.016 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.088 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.096 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
InSb3 (mp-975512) | 0.0000 | 0.243 | 2 |
Rb3Sn (mp-974789) | 0.0000 | 0.152 | 2 |
LiCd3 (mp-973940) | 0.0000 | 0.000 | 2 |
Rb3Sm (mp-974816) | 0.0000 | 0.631 | 2 |
SmAg3 (mp-862736) | 0.0000 | 0.034 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.469 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.136 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Ho_3 |
Final Energy/Atom-1.2402 eV |
Corrected Energy-4.9609 eV
-4.9609 eV = -4.9609 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)