Final Magnetic Moment0.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.040 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRb15Hg16 + Rb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 175.1 |
C (mp-66) | <1 0 0> | <1 0 0> | 101.1 |
C (mp-66) | <1 1 0> | <1 1 0> | 142.9 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 202.2 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 142.9 |
Ge (mp-32) | <1 1 1> | <1 1 1> | 175.1 |
Fe2O3 (mp-24972) | <1 0 0> | <1 1 0> | 142.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 142.9 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 175.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 202.2 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 142.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 202.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 142.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 175.1 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 142.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 101.1 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 101.1 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 142.9 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 175.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
39 | 40 | 40 | 0 | 0 | 0 |
40 | 39 | 40 | 0 | 0 | 0 |
40 | 40 | 39 | 0 | 0 | 0 |
0 | 0 | 0 | 9 | 0 | 0 |
0 | 0 | 0 | 0 | 9 | 0 |
0 | 0 | 0 | 0 | 0 | 9 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-852 | 430.2 | 430.2 | 0 | 0 | 0 |
430.2 | -852 | 430.2 | 0 | 0 | 0 |
430.2 | 430.2 | -852 | 0 | 0 | 0 |
0 | 0 | 0 | 117.2 | 0 | 0 |
0 | 0 | 0 | 0 | 117.2 | 0 |
0 | 0 | 0 | 0 | 0 | 117.2 |
Shear Modulus GV5 GPa |
Bulk Modulus KV39 GPa |
Shear Modulus GR-1 GPa |
Bulk Modulus KR39 GPa |
Shear Modulus GVRH2 GPa |
Bulk Modulus KVRH39 GPa |
Elastic Anisotropy-28.72 |
Poisson's Ratio0.48 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnGaRh2 (mp-977362) | 0.0000 | 0.000 | 3 |
Ba2BeGa (mp-631574) | 0.0000 | 0.584 | 3 |
Zn2NiIr (mp-971836) | 0.0000 | 0.008 | 3 |
Be2PdRh (mp-866115) | 0.0000 | 0.000 | 3 |
Sc2MnSi (mp-999208) | 0.0000 | 0.265 | 3 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
Y3Sn (mp-1094256) | 0.0000 | 0.278 | 2 |
Rb3V (mp-974743) | 0.0000 | 0.927 | 2 |
Cr3Fe (mp-1008282) | 0.0000 | 0.171 | 2 |
Ba3Np (mp-1076925) | 0.0000 | 0.681 | 2 |
Mg3Cd (mp-1038832) | 0.0000 | 0.056 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Hg |
Final Energy/Atom-0.8511 eV |
Corrected Energy-3.4046 eV
-3.4046 eV = -3.4046 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)