material

Re

ID:

mp-975065

DOI:

10.17188/1314713


Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.019 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.019 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
20.51 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Re
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaN (mp-804) <0 0 1> <0 0 1> 0.000 26.9
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.000 87.3
NaCl (mp-22862) <1 1 1> <0 0 1> 0.012 167.9
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.015 53.7
WS2 (mp-224) <1 0 1> <0 0 1> 0.017 322.4
CsI (mp-614603) <1 1 1> <0 0 1> 0.042 107.5
Si (mp-149) <1 1 1> <0 0 1> 0.049 208.2
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.059 208.2
AlN (mp-661) <1 1 1> <0 0 1> 0.074 255.2
CdS (mp-672) <1 0 1> <0 0 1> 0.085 228.4
GaN (mp-804) <1 1 1> <0 0 1> 0.088 214.9
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.100 268.7
SiC (mp-7631) <1 0 1> <0 0 1> 0.113 335.8
MoSe2 (mp-1634) <1 0 1> <0 0 1> 0.114 315.7
InAs (mp-20305) <1 0 0> <0 0 1> 0.117 268.7
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.121 161.2
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.123 20.2
LiF (mp-1138) <1 1 1> <0 0 1> 0.123 87.3
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.134 235.1
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.135 268.7
Mg (mp-153) <1 1 0> <0 0 1> 0.153 201.5
GaN (mp-804) <1 0 0> <1 0 0> 0.155 168.8
ZrO2 (mp-2858) <1 1 -1> <0 0 1> 0.158 181.4
GaP (mp-2490) <1 1 1> <0 0 1> 0.160 208.2
Te2W (mp-22693) <1 1 0> <0 0 1> 0.170 221.7
Ga2O3 (mp-886) <1 1 1> <0 0 1> 0.172 255.2
GaTe (mp-542812) <1 0 0> <0 0 1> 0.185 181.4
Al2O3 (mp-1143) <1 0 0> <0 0 1> 0.186 188.1
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.205 275.4
Fe2O3 (mp-24972) <1 0 0> <0 0 1> 0.245 214.9
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.246 161.2
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.247 214.9
CdWO4 (mp-19387) <1 1 1> <0 0 1> 0.250 208.2
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.274 214.9
ZrO2 (mp-2858) <1 0 1> <0 0 1> 0.278 214.9
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.280 134.3
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.283 127.6
GaSe (mp-1943) <0 0 1> <0 0 1> 0.287 87.3
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.291 208.2
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.293 87.3
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.296 87.3
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.299 241.8
Te2W (mp-22693) <0 1 1> <0 0 1> 0.299 235.1
TeO2 (mp-2125) <0 1 1> <1 0 0> 0.303 225.1
GaP (mp-2490) <1 1 0> <0 0 1> 0.327 214.9
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.331 87.3
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.341 181.4
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.348 168.8
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.352 53.7
TiO2 (mp-390) <1 0 1> <0 0 1> 0.387 275.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
597 278 215 5 0 0
278 597 215 -5 0 0
215 215 670 0 0 0
5 -5 0 151 0 0
0 0 0 0 151 5
0 0 0 0 5 160
Compliance Tensor Sij (10-12Pa-1)
2.2 -0.9 -0.4 -0.1 0 0
-0.9 2.2 -0.4 0.1 0 0
-0.4 -0.4 1.8 0 0 0
-0.1 0.1 0 6.6 0 0
0 0 0 0 6.6 -0.2
0 0 0 0 -0.2 6.3
Shear Modulus GV
169 GPa
Bulk Modulus KV
364 GPa
Shear Modulus GR
165 GPa
Bulk Modulus KR
364 GPa
Shear Modulus GVRH
167 GPa
Bulk Modulus KVRH
364 GPa
Elastic Anisotropy
0.12
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr8Ni50Mo15W2 (mp-767372) 0.2242 0.028 4
CrFeCoNi (mp-1012640) 0.2618 0.065 4
CrFeCoNi (mp-1096923) 0.3756 0.193 4
Mg3In (mp-697180) 0.0659 0.004 2
MgAu3 (mp-30408) 0.1065 0.000 2
HfPd3 (mp-11453) 0.0546 0.000 2
ZrPd3 (mp-30842) 0.0790 0.000 2
HfPt3 (mp-11456) 0.0701 0.000 2
Pr (mp-981544) 0.0125 0.004 1
Li (mp-1018134) 0.0091 0.000 1
Rb (mp-867126) 0.0036 0.024 1
Tb (mp-11698) 0.0029 0.000 1
Ho (mp-10659) 0.0083 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Re_pv
Final Energy/Atom
-12.4260 eV
Corrected Energy
-37.2781 eV
Uncorrected energy = -37.2781 eV Corrected energy = -37.2781 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)