Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.636 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.058 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK2S3 + KC2N3 + C |
Band Gap4.514 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcm [57] |
Hall-P 2c 2b |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 102.4 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 251.9 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 217.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 167.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 337.8 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 72.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 217.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 216.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 253.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 211.1 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 295.5 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 102.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 253.3 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 144.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 337.8 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 42.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 144.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 295.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 42.2 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 288.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 211.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 84.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 211.1 |
BN (mp-984) | <1 1 0> | <1 0 0> | 290.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 337.8 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 167.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 211.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 217.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 216.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 216.5 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 204.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 84.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 253.3 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 211.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 211.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 211.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 253.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 167.2 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 42.2 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 295.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 295.5 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 126.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 126.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 253.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 211.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 42.2 |
TiO2 (mp-2657) | <1 0 0> | <1 1 1> | 110.7 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 102.4 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 168.9 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 295.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbN6Cl (mp-628690) | 0.6916 | 0.111 | 3 |
CsHC2 (mp-31476) | 0.7453 | 0.429 | 3 |
CSO (mp-634755) | 0.6861 | 0.106 | 3 |
CSO (mp-28240) | 0.7088 | 0.105 | 3 |
Cs2CN2 (mp-1029699) | 0.6639 | 0.000 | 3 |
KCSeN (mp-568943) | 0.7006 | 0.115 | 4 |
CsCSN (mp-614311) | 0.5544 | 0.000 | 4 |
SnC2(SN)2 (mp-620404) | 0.6457 | 0.197 | 4 |
TlAg(CN)2 (mp-621981) | 0.6721 | 0.253 | 4 |
KHCN2 (mp-24625) | 0.6849 | 0.011 | 4 |
HgN3 (mp-636839) | 0.4783 | 0.277 | 2 |
CsBr3 (mp-27641) | 0.7133 | 0.000 | 2 |
HgN6 (mp-569461) | 0.6689 | 0.345 | 2 |
HgCl2 (mp-22855) | 0.7406 | 0.000 | 2 |
H3F2 (mp-983357) | 0.6708 | 0.000 | 2 |
K2PtC4(SN)4 (mp-616240) | 0.6039 | 0.379 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv C S N |
Final Energy/Atom-6.0771 eV |
Corrected Energy-99.8873 eV
-99.8873 eV = -97.2334 eV (uncorrected energy) - 2.6538 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)