Final Magnetic Moment0.373 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.186 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.186 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density14.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSc + Pu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 261.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 213.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 251.5 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 284.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 213.4 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 87.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 284.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 213.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 251.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 201.2 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 284.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 251.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 71.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 213.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 201.2 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 251.5 |
BN (mp-984) | <0 0 1> | <1 1 1> | 87.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 150.9 |
BN (mp-984) | <1 1 0> | <1 1 1> | 261.4 |
Al (mp-134) | <1 1 0> | <1 1 0> | 71.1 |
Al (mp-134) | <1 1 1> | <1 1 1> | 87.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 251.5 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 284.5 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 213.4 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 284.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 201.2 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 284.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 50.3 |
C (mp-66) | <1 1 0> | <1 1 0> | 71.1 |
C (mp-66) | <1 1 1> | <1 1 1> | 87.1 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 284.5 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 284.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 174.2 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 251.5 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 251.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 150.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 150.9 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 213.4 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 213.4 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 213.4 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 261.4 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 251.5 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 142.3 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 301.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 284.5 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 213.4 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 251.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 50.3 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 71.1 |
Ni (mp-23) | <1 1 1> | <1 1 1> | 87.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoTmZn2 (mp-983126) | 0.0000 | 0.000 | 3 |
Pm2PtAu (mp-982772) | 0.0000 | 0.000 | 3 |
Nd2IrAu (mp-973606) | 0.0000 | 0.063 | 3 |
YbPrPd2 (mp-981530) | 0.0000 | 0.007 | 3 |
YTmAl2 (mp-980662) | 0.0000 | 0.016 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.164 | 4 |
ErPd (mp-851) | 0.0000 | 0.000 | 2 |
YbRu (mp-567116) | 0.0000 | 0.228 | 2 |
PrIn (mp-20023) | 0.0000 | 0.000 | 2 |
ReC (mp-1009731) | 0.0000 | 1.115 | 2 |
ScCu (mp-1169) | 0.0000 | 0.000 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
U (mp-108) | 0.0000 | 0.271 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pu Sc_sv |
Final Energy/Atom-11.7160 eV |
Corrected Energy-46.8639 eV
-46.8639 eV = -46.8639 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)