Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.001 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKr |
Band Gap7.180 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 230.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 230.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 230.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 88.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 159.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 230.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 212.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 53.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 283.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 283.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 230.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 70.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 230.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 300.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 159.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 353.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 300.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 283.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 283.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 70.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 265.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 212.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 318.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 318.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 230.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 123.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 88.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 336.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 283.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 353.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 212.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 212.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 212.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 283.2 |
Bi2Te3 (mp-34202) | <1 0 0> | <0 0 1> | 141.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 53.1 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 247.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 247.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 70.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 212.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 336.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 70.8 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 300.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 371.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 70.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 212.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 283.2 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 283.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 123.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 17.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.2316 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.2824 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.3873 | 0.193 | 4 |
Mg3In (mp-697180) | 0.0891 | 0.000 | 2 |
MgAu3 (mp-30408) | 0.1223 | 0.000 | 2 |
HfPd3 (mp-11453) | 0.0614 | 0.000 | 2 |
ZrPd3 (mp-30842) | 0.0902 | 0.000 | 2 |
HfPt3 (mp-11456) | 0.0781 | 0.000 | 2 |
Yb (mp-972364) | 0.0116 | 0.000 | 1 |
Ag (mp-989737) | 0.0030 | 0.000 | 1 |
Ag (mp-8566) | 0.0209 | 0.007 | 1 |
Mo (mp-1066523) | 0.0208 | 0.442 | 1 |
Gd (mp-570087) | 0.0171 | 0.020 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Kr |
Final Energy/Atom-0.0562 eV |
Corrected Energy-0.1686 eV
-0.1686 eV = -0.1686 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)