Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.271 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 292.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 125.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 102.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 143.3 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 326.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 266.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 225.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 307.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 307.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 163.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 40.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 167.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 204.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 225.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 143.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 102.4 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 232.9 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 59.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 266.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 307.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 232.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 348.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 40.9 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 292.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 184.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 163.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 313.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 266.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 81.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 327.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 266.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 348.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 251.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 81.9 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 232.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 102.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 59.2 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 292.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 81.9 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 334.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 102.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 125.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 204.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 266.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 177.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 313.1 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 295.9 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 236.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 326.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 40.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
82 | 50 | 29 | 0 | 0 | 0 |
50 | 82 | 29 | 0 | 0 | 0 |
29 | 29 | 92 | 0 | 0 | 0 |
0 | 0 | 0 | 24 | 0 | 0 |
0 | 0 | 0 | 0 | 24 | 0 |
0 | 0 | 0 | 0 | 0 | 18 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
19.8 | -11 | -2.8 | 0 | 0 | 0 |
-11 | 19.8 | -2.8 | 0 | 0 | 0 |
-2.8 | -2.8 | 12.6 | 0 | 0 | 0 |
0 | 0 | 0 | 40.8 | 0 | 0 |
0 | 0 | 0 | 0 | 40.8 | 0 |
0 | 0 | 0 | 0 | 0 | 56.3 |
Shear Modulus GV23 GPa |
Bulk Modulus KV52 GPa |
Shear Modulus GR22 GPa |
Bulk Modulus KR52 GPa |
Shear Modulus GVRH23 GPa |
Bulk Modulus KVRH52 GPa |
Elastic Anisotropy0.35 |
Poisson's Ratio0.31 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
USbTe (mp-7935) | 0.1785 | 0.000 | 3 |
ThAsSe (mp-1019357) | 0.1565 | 0.000 | 3 |
ThBiTe (mp-1019362) | 0.1906 | 0.000 | 3 |
NpSbTe (mp-1018824) | 0.1806 | 0.000 | 3 |
ThPS (mp-12876) | 0.1247 | 0.000 | 3 |
ErSe2 (mp-9978) | 0.0310 | 0.041 | 2 |
LuSe2 (mp-1018793) | 0.0280 | 0.082 | 2 |
DySe2 (mp-1018683) | 0.0392 | 0.020 | 2 |
TmSe2 (mp-1072474) | 0.0283 | 0.055 | 2 |
NdTe2 (mp-2550) | 0.0096 | 0.002 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pr_3 Te |
Final Energy/Atom-4.9603 eV |
Corrected Energy-29.7616 eV
-29.7616 eV = -29.7616 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)