Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.242 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.242 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density0.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi + Be |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 227.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 161.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 236.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 220.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 43.1 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 129.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 91.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 190.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 183.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 220.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 86.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 215.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 227.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 190.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 305.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 234.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 161.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 190.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 213.5 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 236.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 169.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 91.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 215.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 91.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 129.4 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 270.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 44.0 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 301.9 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 129.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 129.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 236.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 244.0 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 169.2 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 301.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 43.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 220.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 278.9 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 129.4 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 91.5 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 236.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 73.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 91.5 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 335.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 264.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 91.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 322.9 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 244.0 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 227.8 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 172.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
19 | 19 | 24 | 0 | 0 | 0 |
19 | 19 | 24 | 0 | 0 | 0 |
24 | 24 | 34 | 0 | 0 | 0 |
0 | 0 | 0 | 26 | 0 | 0 |
0 | 0 | 0 | 0 | 26 | 0 |
0 | 0 | 0 | 0 | 0 | 20 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4332 | -4163.5 | -115.8 | 0 | 0 | 0 |
-4163.5 | 4332 | -115.8 | 0 | 0 | 0 |
-115.8 | -115.8 | 188.2 | 0 | 0 | 0 |
0 | 0 | 0 | 38.5 | 0 | 0 |
0 | 0 | 0 | 0 | 38.5 | 0 |
0 | 0 | 0 | 0 | 0 | 49.8 |
Shear Modulus GV15 GPa |
Bulk Modulus KV23 GPa |
Shear Modulus GR0 GPa |
Bulk Modulus KR16 GPa |
Shear Modulus GVRH8 GPa |
Bulk Modulus KVRH20 GPa |
Elastic Anisotropy259.38 |
Poisson's Ratio0.33 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.0766 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.1686 | 0.034 | 3 |
GaFeNi2 (mp-1065359) | 0.1710 | 0.065 | 3 |
MnGaFe2 (mp-1065753) | 0.1674 | 0.037 | 3 |
GaCo2Ni (mp-1018060) | 0.1815 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.1884 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3146 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3623 | 0.193 | 4 |
Yb3U (mp-979951) | 0.0096 | 0.633 | 2 |
SbPt3 (mp-973354) | 0.0111 | 0.119 | 2 |
LiCu3 (mp-862658) | 0.0160 | 0.000 | 2 |
Cr3Fe (mp-1017511) | 0.0001 | 0.270 | 2 |
LiAg (mp-1018026) | 0.0025 | 0.001 | 2 |
In (mp-85) | 0.0521 | 0.037 | 1 |
Na (mp-974920) | 0.1373 | 0.005 | 1 |
Tl (mp-151) | 0.1255 | 0.010 | 1 |
La (mp-156) | 0.0808 | 0.001 | 1 |
Sn (mp-623511) | 0.1278 | 0.061 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Be_sv |
Final Energy/Atom-2.1249 eV |
Corrected Energy-8.4995 eV
-8.4995 eV = -8.4995 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)