Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.308 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.328 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNdS2 + S |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <0 0 1> | <0 0 1> | 200.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 325.9 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 217.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 344.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 260.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 32.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 114.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 28.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 316.5 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 260.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 293.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 258.0 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 303.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 344.0 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 293.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 86.0 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 97.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 28.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 114.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 86.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 86.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 97.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 200.7 |
BN (mp-984) | <1 1 0> | <1 0 1> | 130.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 200.7 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 303.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 200.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 114.7 |
Al (mp-134) | <1 0 0> | <1 0 0> | 32.6 |
Al (mp-134) | <1 1 0> | <1 1 0> | 112.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 28.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 217.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 1> | 63.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 169.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 293.3 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 189.9 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 303.8 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 32.6 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 282.2 |
TeO2 (mp-2125) | <0 1 1> | <1 1 0> | 225.8 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 282.2 |
TeO2 (mp-2125) | <1 0 1> | <1 1 0> | 225.8 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 217.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 200.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 344.0 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 217.0 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 217.0 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 130.3 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 217.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 195.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaMg14Ni (mp-1099078) | 0.5872 | 0.190 | 3 |
LuO3 (mp-973457) | 0.1506 | 0.560 | 2 |
DyO3 (mp-984359) | 0.2533 | 0.504 | 2 |
PrS3 (mp-975653) | 0.0298 | 0.322 | 2 |
UP3 (mp-865428) | 0.3127 | 0.000 | 2 |
AcSe3 (mp-867800) | 0.1271 | 0.007 | 2 |
Mn (mp-542909) | 0.5381 | 0.055 | 1 |
N2 (mp-672234) | 0.3998 | 0.000 | 1 |
W (mp-1065340) | 0.4874 | 0.491 | 1 |
Cd (mp-94) | 0.4039 | 0.000 | 1 |
Zn (mp-79) | 0.4043 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 S |
Final Energy/Atom-5.1043 eV |
Corrected Energy-44.8153 eV
-44.8153 eV = -40.8345 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)