Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.181 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.181 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAc + Li |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 342.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 365.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 261.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 342.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 182.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 235.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 329.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 141.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 261.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 274.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 297.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 342.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 329.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 297.1 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 140.8 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 199.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 209.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 182.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 228.5 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 329.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 182.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 329.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 114.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 114.3 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 266.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 91.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 266.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 365.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 297.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 205.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 114.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 274.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 205.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 114.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 235.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 235.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 329.6 |
BN (mp-984) | <1 1 1> | <1 0 0> | 329.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 266.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 209.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 182.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 205.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 209.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 342.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 205.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 297.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 182.8 |
MoS2 (mp-1434) | <1 0 0> | <1 0 1> | 209.3 |
MoS2 (mp-1434) | <1 0 1> | <1 0 1> | 209.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 205.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
11 | 34 | 4 | 0 | 0 | 0 |
34 | 11 | 4 | 0 | 0 | 0 |
4 | 4 | 28 | 0 | 0 | 0 |
0 | 0 | 0 | 13 | 0 | 0 |
0 | 0 | 0 | 0 | 13 | 0 |
0 | 0 | 0 | 0 | 0 | 30 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-10.2 | 33.3 | -3.5 | 0 | 0 | 0 |
33.3 | -10.2 | -3.5 | 0 | 0 | 0 |
-3.5 | -3.5 | 36.7 | 0 | 0 | 0 |
0 | 0 | 0 | 76 | 0 | 0 |
0 | 0 | 0 | 0 | 76 | 0 |
0 | 0 | 0 | 0 | 0 | 33.3 |
Shear Modulus GV12 GPa |
Bulk Modulus KV15 GPa |
Shear Modulus GR29 GPa |
Bulk Modulus KR15 GPa |
Shear Modulus GVRH20 GPa |
Bulk Modulus KVRH15 GPa |
Elastic Anisotropy-2.95 |
Poisson's Ratio0.03 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.0218 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.1163 | 0.034 | 3 |
LiCa6Ge (mp-12609) | 0.1343 | 0.183 | 3 |
GaFeNi2 (mp-1065359) | 0.1178 | 0.065 | 3 |
GaCo2Ni (mp-1018060) | 0.1270 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.1771 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3174 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3644 | 0.193 | 4 |
ScRu3 (mp-973022) | 0.0091 | 0.242 | 2 |
Tl3V (mp-981210) | 0.0068 | 0.508 | 2 |
Rb3Ca (mp-975043) | 0.0002 | 0.201 | 2 |
Rb3Lu (mp-974966) | 0.0051 | 0.624 | 2 |
RbSr3 (mp-975222) | 0.0091 | 0.137 | 2 |
In (mp-85) | 0.1069 | 0.037 | 1 |
Pr (mp-97) | 0.1162 | 0.008 | 1 |
Ce (mp-567332) | 0.1181 | 0.000 | 1 |
Rb (mp-12628) | 0.1096 | 0.015 | 1 |
La (mp-156) | 0.0261 | 0.001 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ac |
Final Energy/Atom-2.2806 eV |
Corrected Energy-9.1225 eV
-9.1225 eV = -9.1225 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)