Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.370 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.186 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHoSb + Sb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 333.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 213.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 268.9 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 199.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 148.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.2 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 228.5 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 332.7 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 266.1 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 66.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 185.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 259.6 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 266.9 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 133.1 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 266.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 148.3 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 213.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 115.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 185.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 228.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 199.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 266.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 185.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 115.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 266.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 259.6 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 66.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 185.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 111.2 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 66.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 192.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 115.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 111.2 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 228.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 268.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 185.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 111.2 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 192.1 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 213.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 296.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 333.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 268.9 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 192.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 259.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 148.3 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 115.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 268.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 37.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 148.3 |
BN (mp-984) | <1 0 1> | <1 0 1> | 266.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrFeCoNi (mp-1012640) | 0.6565 | 0.057 | 4 |
Pa3Ta (mp-973815) | 0.1382 | 0.184 | 2 |
Pa3Mo (mp-1006127) | 0.0833 | 0.221 | 2 |
Pa3Nb (mp-983550) | 0.1238 | 0.171 | 2 |
LuSb3 (mp-973615) | 0.0972 | 0.220 | 2 |
NpSb3 (mp-977296) | 0.1251 | 0.002 | 2 |
Cr8Ni50Mo17 (mp-766895) | 0.7122 | 0.027 | 3 |
YEr4Al15 (mp-979428) | 0.7471 | 0.001 | 3 |
Cr11Ni40Mo9 (mp-766580) | 0.7005 | 0.019 | 3 |
Zn2CuAu (mp-12759) | 0.5847 | 0.000 | 3 |
Xe (mp-972256) | 0.5506 | 0.000 | 1 |
Ce (mp-20736) | 0.4673 | 0.089 | 1 |
Cr (mp-89) | 0.4513 | 0.408 | 1 |
Ho (mp-144) | 0.5879 | 0.000 | 1 |
Tl (mp-972351) | 0.4153 | 0.014 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points28 |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 Sb |
Final Energy/Atom-4.6082 eV |
Corrected Energy-36.8658 eV
-36.8658 eV = -36.8658 eV (uncorrected energy)
|