Final Magnetic Moment0.073 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.141 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.56 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi5Sb2 + Ni |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 124.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 176.7 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 216.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 69.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 176.7 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 168.3 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 120.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 58.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 72.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 166.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 83.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 208.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 58.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 124.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 249.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 333.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 291.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 353.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 157.1 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 120.2 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 58.9 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 72.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 24.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 137.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 72.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 117.8 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 120.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 124.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 176.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 176.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 333.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 124.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 41.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 137.4 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 176.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 78.5 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 196.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 180.5 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 157.1 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 333.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 176.7 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 168.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 124.9 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 78.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 291.5 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 319.3 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 157.1 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 157.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 69.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 69.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
222 | 146 | 146 | 0 | 0 | 0 |
146 | 222 | 146 | 0 | 0 | 0 |
146 | 146 | 222 | 0 | 0 | 0 |
0 | 0 | 0 | 58 | 0 | 0 |
0 | 0 | 0 | 0 | 58 | 0 |
0 | 0 | 0 | 0 | 0 | 58 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
9.5 | -3.8 | -3.8 | 0 | 0 | 0 |
-3.8 | 9.5 | -3.8 | 0 | 0 | 0 |
-3.8 | -3.8 | 9.5 | 0 | 0 | 0 |
0 | 0 | 0 | 17.2 | 0 | 0 |
0 | 0 | 0 | 0 | 17.2 | 0 |
0 | 0 | 0 | 0 | 0 | 17.2 |
Shear Modulus GV50 GPa |
Bulk Modulus KV171 GPa |
Shear Modulus GR48 GPa |
Bulk Modulus KR171 GPa |
Shear Modulus GVRH49 GPa |
Bulk Modulus KVRH171 GPa |
Elastic Anisotropy0.23 |
Poisson's Ratio0.37 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
YHo3 (mp-980082) | 0.0000 | 0.030 | 2 |
NdDy3 (mp-975388) | 0.0000 | 0.019 | 2 |
Pt3Rh (mp-974395) | 0.0000 | 0.004 | 2 |
LuRh3 (mp-865802) | 0.0000 | 0.000 | 2 |
TiPd3 (mp-636328) | 0.0000 | 0.009 | 2 |
P (mp-674158) | 0.0000 | 3.518 | 1 |
Xe (mp-611517) | 0.0000 | 0.006 | 1 |
Eu (mp-623532) | 0.0000 | 0.035 | 1 |
He (mp-614456) | 0.0000 | 0.008 | 1 |
Au (mp-81) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ni_pv Sb |
Final Energy/Atom-5.5079 eV |
Corrected Energy-22.0317 eV
-22.0317 eV = -22.0317 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)