Final Magnetic Moment0.822 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.814 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.814 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa + Ru |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 75.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 215.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 75.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 129.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 75.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 240.0 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 237.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 195.0 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 169.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 43.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 213.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 135.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 75.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 169.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 45.0 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 169.7 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 301.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 165.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 86.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 305.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 240.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 195.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 237.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 195.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 172.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 43.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 91.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 60.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 129.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 215.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 225.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 285.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 75.0 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 271.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 135.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 129.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 91.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 225.0 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 228.0 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 301.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 300.0 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 258.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 135.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 255.0 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 271.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 330.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 270.0 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 300.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 255.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
193 | 158 | 158 | 0 | 0 | 0 |
158 | 193 | 158 | 0 | 0 | 0 |
158 | 158 | 215 | 0 | 0 | 0 |
0 | 0 | 0 | 70 | 0 | 0 |
0 | 0 | 0 | 0 | 70 | 0 |
0 | 0 | 0 | 0 | 0 | 69 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
18.7 | -10.2 | -6.2 | 0 | 0 | 0 |
-10.2 | 18.7 | -6.2 | 0 | 0 | 0 |
-6.2 | -6.2 | 13.8 | 0 | 0 | 0 |
0 | 0 | 0 | 14.3 | 0 | 0 |
0 | 0 | 0 | 0 | 14.3 | 0 |
0 | 0 | 0 | 0 | 0 | 14.4 |
Shear Modulus GV50 GPa |
Bulk Modulus KV172 GPa |
Shear Modulus GR35 GPa |
Bulk Modulus KR172 GPa |
Shear Modulus GVRH43 GPa |
Bulk Modulus KVRH172 GPa |
Elastic Anisotropy2.11 |
Poisson's Ratio0.39 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.0640 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0471 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0486 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0435 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0424 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.1921 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3399 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.3837 | 0.193 | 4 |
K3In (mp-982664) | 0.0016 | 0.123 | 2 |
KLa3 (mp-973250) | 0.0029 | 0.428 | 2 |
Na3Be (mp-977194) | 0.0001 | 0.510 | 2 |
Li3Cu (mp-975882) | 0.0016 | 0.022 | 2 |
Hf3Mg (mp-1094220) | 0.0001 | 0.084 | 2 |
Pr (mp-97) | 0.0434 | 0.008 | 1 |
Sc (mp-36) | 0.0452 | 0.049 | 1 |
Sm (mp-21377) | 0.0408 | 0.010 | 1 |
Hg (mp-753304) | 0.0445 | 0.012 | 1 |
Th (mp-37) | 0.0421 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Ru_pv |
Final Energy/Atom-6.4694 eV |
Corrected Energy-25.8776 eV
-25.8776 eV = -25.8776 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)