Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom0.174 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.174 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHg + Sb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 181.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 254.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 64.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 181.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 36.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 224.6 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 156.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 181.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 145.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 223.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 194.5 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 208.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 290.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 64.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 181.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 223.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 181.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 112.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 260.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 254.5 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 64.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 181.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 64.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 181.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 109.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 109.1 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 260.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 299.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 262.1 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 260.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 181.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 109.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 112.3 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 324.2 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 299.5 |
Te2W (mp-22693) | <1 0 1> | <1 0 1> | 104.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 187.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 260.9 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 208.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 299.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 145.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 337.0 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 187.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 254.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 259.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 260.9 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 112.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 262.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 218.1 |
BN (mp-984) | <1 0 1> | <1 0 1> | 260.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrFeCoNi (mp-1012640) | 0.6408 | 0.057 | 4 |
Tl3Br (mp-982064) | 0.0833 | 0.159 | 2 |
PaPd3 (mp-862854) | 0.0980 | 0.000 | 2 |
Tl3Cl (mp-983458) | 0.0630 | 0.176 | 2 |
Si3B (mp-972733) | 0.0978 | 0.923 | 2 |
VMo (mp-995205) | 0.0581 | 0.391 | 2 |
Cr7Ni20Mo3 (mp-768654) | 0.7387 | 0.014 | 3 |
Cr8Ni50Mo17 (mp-766895) | 0.7135 | 0.027 | 3 |
Cr11Ni40Mo9 (mp-766580) | 0.7246 | 0.019 | 3 |
Zn2CuAu (mp-12759) | 0.6185 | 0.000 | 3 |
Xe (mp-972256) | 0.3252 | 0.000 | 1 |
Ce (mp-20736) | 0.1002 | 0.089 | 1 |
Cr (mp-89) | 0.0619 | 0.408 | 1 |
Ho (mp-144) | 0.4242 | 0.000 | 1 |
Tl (mp-972351) | 0.3274 | 0.014 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points28 |
U Values-- |
PseudopotentialsVASP PAW: Hg Sb |
Final Energy/Atom-1.0851 eV |
Corrected Energy-8.6811 eV
-8.6811 eV = -8.6811 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)