Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.726 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 231.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 231.9 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 328.0 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 328.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 231.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 131.2 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 262.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 196.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 241.0 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 80.3 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 262.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 328.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 160.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 278.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 185.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 196.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 241.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 139.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 139.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 196.8 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 262.4 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 324.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 231.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 231.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 231.9 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 196.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 262.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 231.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 231.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 231.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 241.0 |
Al (mp-134) | <1 1 1> | <1 0 0> | 139.2 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 328.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 328.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 46.4 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 65.6 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 80.3 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 196.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 92.8 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 231.9 |
C (mp-66) | <1 0 0> | <1 0 0> | 231.9 |
C (mp-66) | <1 1 0> | <1 1 0> | 196.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 1> | 160.7 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 278.3 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 262.4 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 231.9 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 231.9 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 185.5 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 196.8 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 241.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NdInPd2 (mp-977590) | 0.0000 | 0.013 | 3 |
Pr2MgTl (mp-861505) | 0.0000 | 0.006 | 3 |
Ti2ReIr (mp-865717) | 0.0000 | 0.000 | 3 |
LiDyTl2 (mp-867108) | 0.0000 | 0.000 | 3 |
LiCa2Tl (mp-867167) | 0.0000 | 0.000 | 3 |
TiFeCoAs (mp-998974) | 0.0000 | 0.146 | 4 |
TiGaFeCo (mp-998964) | 0.0000 | 0.000 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.198 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.009 | 4 |
Yb3V (mp-979942) | 0.0000 | 0.453 | 2 |
Na3Ca (mp-977062) | 0.0000 | 0.087 | 2 |
NaTm3 (mp-976863) | 0.0000 | 0.325 | 2 |
Li3Mg (mp-976256) | 0.0000 | 0.010 | 2 |
ScTc3 (mp-867262) | 0.0000 | 0.118 | 2 |
Xe (mp-979285) | 0.0000 | 0.002 | 1 |
Cu (mp-998890) | 0.0000 | 0.035 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.346 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Cd Pd |
Final Energy/Atom-4.7031 eV |
Corrected Energy-18.8123 eV
-18.8123 eV = -18.8123 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)