Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.488 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 264.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 190.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 343.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 152.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 161.9 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 198.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 305.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 38.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 54.0 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 66.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 190.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 190.8 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 269.8 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 323.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 152.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 66.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 267.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 343.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 305.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 38.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 54.0 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 66.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 305.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 198.2 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 198.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 152.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 215.8 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 198.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 107.9 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 264.3 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 190.8 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 190.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 343.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 267.1 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 264.3 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 190.8 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 190.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 152.6 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 215.8 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 264.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 267.1 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 54.0 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 66.1 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 305.2 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 264.3 |
BN (mp-984) | <0 0 1> | <1 1 1> | 66.1 |
BN (mp-984) | <1 0 1> | <1 0 0> | 305.2 |
BN (mp-984) | <1 1 0> | <1 1 1> | 66.1 |
BN (mp-984) | <1 1 1> | <1 0 0> | 267.1 |
C (mp-48) | <0 0 1> | <1 0 0> | 190.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
378 | 229 | 229 | 0 | 0 | 0 |
229 | 378 | 229 | 0 | 0 | 0 |
229 | 229 | 378 | 0 | 0 | 0 |
0 | 0 | 0 | 118 | 0 | 0 |
0 | 0 | 0 | 0 | 118 | 0 |
0 | 0 | 0 | 0 | 0 | 118 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.9 | -1.8 | -1.8 | 0 | 0 | 0 |
-1.8 | 4.9 | -1.8 | 0 | 0 | 0 |
-1.8 | -1.8 | 4.9 | 0 | 0 | 0 |
0 | 0 | 0 | 8.4 | 0 | 0 |
0 | 0 | 0 | 0 | 8.4 | 0 |
0 | 0 | 0 | 0 | 0 | 8.4 |
Shear Modulus GV101 GPa |
Bulk Modulus KV279 GPa |
Shear Modulus GR96 GPa |
Bulk Modulus KR279 GPa |
Shear Modulus GVRH98 GPa |
Bulk Modulus KVRH279 GPa |
Elastic Anisotropy0.26 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
PrSmTl2 (mp-975920) | 0.0000 | 0.001 | 3 |
LiSbRh2 (mp-861667) | 0.0000 | 0.000 | 3 |
PmNi2Sn (mp-862952) | 0.0000 | 0.000 | 3 |
Yb2AgGe (mp-865630) | 0.0000 | 0.000 | 3 |
SmZn2Ag (mp-867140) | 0.0000 | 0.022 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
PbAu3 (mp-982246) | 0.0000 | 0.082 | 2 |
FeAg3 (mp-973533) | 0.0000 | 0.347 | 2 |
ZnSn3 (mp-980905) | 0.0000 | 0.127 | 2 |
Ta3Ru (mp-977390) | 0.0000 | 0.000 | 2 |
Tl3Si (mp-972082) | 0.0000 | 0.344 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Nb_pv Ir |
Final Energy/Atom-7.9095 eV |
Corrected Energy-31.6379 eV
-31.6379 eV = -31.6379 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)