Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.454 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHo2S3 |
Band Gap2.634 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [167] |
Hall-R 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 163.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 286.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 327.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 122.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 133.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 286.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 286.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 204.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 163.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 163.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 163.5 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 122.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 204.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 286.2 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 286.2 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 204.4 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 163.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 286.2 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 204.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 122.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 204.4 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 286.2 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 122.6 |
Ga2O3 (mp-886) | <0 1 0> | <0 0 1> | 286.2 |
Si (mp-149) | <1 1 1> | <0 0 1> | 163.5 |
Au (mp-81) | <1 0 0> | <0 0 1> | 204.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 122.6 |
C (mp-48) | <0 0 1> | <0 0 1> | 163.5 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 286.2 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 286.2 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 122.6 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 0> | 253.4 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 327.1 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 122.6 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 286.2 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 204.4 |
MgAl2O4 (mp-3536) | <1 1 1> | <0 0 1> | 122.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 163.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 163.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 286.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 204.4 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 163.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 286.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 163.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 253.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 286.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 245.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 204.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 286.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 204.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VCrO3 (mp-775827) | 0.0945 | 0.034 | 3 |
VCrO3 (mp-770779) | 0.0883 | 0.031 | 3 |
VCrO3 (mp-770843) | 0.0941 | 0.007 | 3 |
VCrO3 (mp-770778) | 0.0888 | 0.034 | 3 |
VCrO3 (mp-768065) | 0.0918 | 0.721 | 3 |
Mg2VWO6 (mvc-5881) | 0.3627 | 0.018 | 4 |
Mg2TiWO6 (mvc-5939) | 0.3949 | 0.128 | 4 |
Mg2CrWO6 (mvc-5960) | 0.3840 | 0.047 | 4 |
InNi2SbO6 (mp-1078367) | 0.2868 | 0.000 | 4 |
ScNi2SbO6 (mp-1078244) | 0.3162 | 0.000 | 4 |
Mn2O3 (mp-770543) | 0.0527 | 0.064 | 2 |
Cr2O3 (mp-796301) | 0.0310 | 0.000 | 2 |
Tm2S3 (mp-14787) | 0.0322 | 0.020 | 2 |
Cr2O3 (mp-19399) | 0.0303 | 0.000 | 2 |
Rh2O3 (mp-542734) | 0.0421 | 0.027 | 2 |
Li4Fe2TeWO12 (mp-768021) | 0.6377 | 0.083 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.7116 | 0.054 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 S |
Final Energy/Atom-6.3712 eV |
Corrected Energy-67.6929 eV
-67.6929 eV = -63.7121 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)