Final Magnetic Moment3.076 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.979 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.290 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 298.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 298.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 298.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 298.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 128.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 139.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 54.1 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 100.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 286.5 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 209.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 128.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 85.3 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 298.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 209.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 213.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 139.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 54.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 250.1 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 209.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 128.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 139.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 128.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 69.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 270.6 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 162.4 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 69.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 341.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 213.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 270.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 270.6 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 299.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 213.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 213.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 298.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 298.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 298.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 170.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 255.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 128.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 255.9 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 128.0 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 69.7 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 69.7 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 298.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 213.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 213.3 |
MoS2 (mp-1434) | <1 0 0> | <1 1 1> | 199.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 128.0 |
Al (mp-134) | <1 1 0> | <1 0 1> | 69.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 255.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb2RuO4 (mp-542697) | 0.6194 | 0.000 | 3 |
Cs2TeO4 (mp-669353) | 0.5957 | 0.000 | 3 |
Rb2MgH4 (mp-643770) | 0.6206 | 0.013 | 3 |
K2CrO4 (mp-19232) | 0.6084 | 0.000 | 3 |
Rb2SeO4 (mp-4618) | 0.5997 | 0.000 | 3 |
K3Sm(PO4)2 (mp-18019) | 0.1235 | 0.000 | 4 |
K3La(PO4)2 (mp-1019793) | 0.1702 | 0.000 | 4 |
K3Eu(PO4)2 (mp-17089) | 0.1091 | 0.237 | 4 |
K3Nd(PO4)2 (mp-17187) | 0.1054 | 0.000 | 4 |
K3Ce(PO4)2 (mp-17189) | 0.1353 | 0.000 | 4 |
K2UP2(H2O5)2 (mp-722535) | 0.6890 | 0.377 | 5 |
K2USO7F2 (mp-863004) | 0.5431 | 0.185 | 5 |
K2SbSO4F3 (mp-554643) | 0.6138 | 0.000 | 5 |
RbUSO6F (mp-560102) | 0.7375 | 0.000 | 5 |
SrCaP2WO8 (mvc-3024) | 0.6951 | 0.266 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Gd P O |
Final Energy/Atom-7.4231 eV |
Corrected Energy-218.8375 eV
Uncorrected energy = -207.8455 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Corrected energy = -218.8375 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)