Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.417 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.004 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 222.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 294.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 159.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 196.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 318.1 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 154.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 159.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 318.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.5 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 278.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 318.1 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 270.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 159.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 79.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 357.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 222.7 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 270.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 198.8 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 357.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 270.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 159.0 |
Ag (mp-124) | <1 1 1> | <1 0 -1> | 270.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 67.5 |
BN (mp-984) | <0 0 1> | <1 0 1> | 98.1 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 67.5 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 159.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 278.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 198.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 357.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 202.5 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 294.4 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 357.8 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 357.8 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 294.4 |
CeO2 (mp-20194) | <1 1 1> | <1 0 -1> | 202.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 278.3 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 278.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 198.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 159.0 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 357.8 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 357.8 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 357.8 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 196.3 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 196.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 297.0 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 357.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 222.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 270.0 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 297.0 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 198.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KSm2Cl5 (mp-568044) | 0.4316 | 0.091 | 3 |
CsAg3Se2 (mp-16234) | 0.3052 | 0.000 | 3 |
RbAg3Se2 (mp-10477) | 0.2012 | 0.000 | 3 |
RbAg3Te2 (mp-10481) | 0.3822 | 0.000 | 3 |
TlCu3Se2 (mp-8800) | 0.4515 | 0.027 | 3 |
K2BaCdSb2 (mp-863761) | 0.7490 | 0.000 | 4 |
K2SrCdSb2 (mp-863758) | 0.7179 | 0.000 | 4 |
Gd3NbS3O4 (mp-510057) | 0.6757 | 0.062 | 4 |
KSr2Cd2Sb3 (mp-866639) | 0.5635 | 0.000 | 4 |
Sm3NbS3O4 (mp-16135) | 0.7299 | 0.004 | 4 |
K4Sn9 (mp-570900) | 0.4667 | 0.000 | 2 |
Mg2Si3 (mp-1073157) | 0.4798 | 0.236 | 2 |
Mg2Si3 (mp-1073224) | 0.4741 | 0.182 | 2 |
MgSi (mp-1073735) | 0.4668 | 0.204 | 2 |
Mg3Si4 (mp-1075198) | 0.5007 | 0.266 | 2 |
Rb (mp-640416) | 0.5245 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Ag Se |
Final Energy/Atom-3.1839 eV |
Corrected Energy-38.2070 eV
-38.2070 eV = -38.2070 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)