Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.043 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.043 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSm + Th |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 177.0 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 108.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 281.0 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 361.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 229.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 325.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 127.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 144.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 108.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 204.3 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 177.0 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 108.4 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 177.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 204.3 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 325.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 281.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 127.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 178.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 108.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 281.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 108.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 204.3 |
BN (mp-984) | <0 0 1> | <1 1 0> | 108.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 76.6 |
BN (mp-984) | <1 0 1> | <1 0 0> | 255.4 |
BN (mp-984) | <1 1 0> | <1 1 0> | 325.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 289.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 127.7 |
InAs (mp-20305) | <1 0 0> | <1 1 1> | 309.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 108.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 309.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 76.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 127.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 144.5 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 177.0 |
Al (mp-134) | <1 1 0> | <1 1 0> | 72.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 108.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 127.7 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 0> | 289.0 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 309.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 127.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 72.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 144.5 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 127.7 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 132.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 76.6 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 252.9 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 325.1 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 144.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 127.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
78 | 42 | 42 | 0 | 0 | 0 |
42 | 78 | 42 | 0 | 0 | 0 |
42 | 42 | 78 | 0 | 0 | 0 |
0 | 0 | 0 | 46 | 0 | 0 |
0 | 0 | 0 | 0 | 46 | 0 |
0 | 0 | 0 | 0 | 0 | 46 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
20.8 | -7.3 | -7.3 | 0 | 0 | 0 |
-7.3 | 20.8 | -7.3 | 0 | 0 | 0 |
-7.3 | -7.3 | 20.8 | 0 | 0 | 0 |
0 | 0 | 0 | 21.8 | 0 | 0 |
0 | 0 | 0 | 0 | 21.8 | 0 |
0 | 0 | 0 | 0 | 0 | 21.8 |
Shear Modulus GV35 GPa |
Bulk Modulus KV54 GPa |
Shear Modulus GR28 GPa |
Bulk Modulus KR54 GPa |
Shear Modulus GVRH31 GPa |
Bulk Modulus KVRH54 GPa |
Elastic Anisotropy1.16 |
Poisson's Ratio0.26 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
Ga3Bi (mp-983237) | 0.0000 | 0.072 | 2 |
Sc3Al (mp-978498) | 0.0000 | 0.021 | 2 |
Rb3Ag (mp-975051) | 0.0000 | 0.136 | 2 |
Tm3P (mp-971958) | 0.0000 | 0.488 | 2 |
HgPd3 (mp-863720) | 0.0000 | 0.020 | 2 |
U (mp-1008669) | 0.0000 | 0.372 | 1 |
Rh (mp-74) | 0.0000 | 0.000 | 1 |
Pb (mp-20483) | 0.0000 | 0.000 | 1 |
Mg (mp-1056702) | 0.0000 | 0.014 | 1 |
N2 (mp-1056857) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Th |
Final Energy/Atom-6.6971 eV |
Corrected Energy-26.7883 eV
-26.7883 eV = -26.7883 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)