Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.394 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToY2Al + YAl2 + SmAl |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 1> | 276.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 265.6 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 276.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 265.6 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 150.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 212.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 225.4 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 276.0 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 276.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 159.4 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 225.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 265.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 212.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 53.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 318.7 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 212.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 225.4 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 276.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 265.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 225.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 265.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 265.6 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 225.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 75.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 265.6 |
BN (mp-984) | <1 1 0> | <1 1 1> | 276.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 265.6 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 225.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 265.6 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 150.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 212.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 212.5 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 265.6 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 225.4 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 225.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 212.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 265.6 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 225.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 212.5 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 225.4 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 92.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 276.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 159.4 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 75.1 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 92.0 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 318.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 225.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 265.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 265.6 |
C (mp-66) | <1 1 1> | <1 0 0> | 265.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
80 | 54 | 54 | 0 | 0 | 0 |
54 | 80 | 54 | 0 | 0 | 0 |
54 | 54 | 80 | 0 | 0 | 0 |
0 | 0 | 0 | 62 | 0 | 0 |
0 | 0 | 0 | 0 | 62 | 0 |
0 | 0 | 0 | 0 | 0 | 62 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
26.8 | -10.7 | -10.7 | 0 | 0 | 0 |
-10.7 | 26.8 | -10.7 | 0 | 0 | 0 |
-10.7 | -10.7 | 26.8 | 0 | 0 | 0 |
0 | 0 | 0 | 16 | 0 | 0 |
0 | 0 | 0 | 0 | 16 | 0 |
0 | 0 | 0 | 0 | 0 | 16 |
Shear Modulus GV43 GPa |
Bulk Modulus KV63 GPa |
Shear Modulus GR25 GPa |
Bulk Modulus KR63 GPa |
Shear Modulus GVRH34 GPa |
Bulk Modulus KVRH63 GPa |
Elastic Anisotropy3.48 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CdSnRh2 (mp-861877) | 0.0000 | 0.000 | 3 |
CaPmCd2 (mp-862881) | 0.0000 | 0.000 | 3 |
Pm2AgSn (mp-862990) | 0.0000 | 0.000 | 3 |
NaNdAu2 (mp-865113) | 0.0000 | 0.013 | 3 |
LiCd2Pd (mp-867196) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
ZnHg3 (mp-971757) | 0.0000 | 0.122 | 2 |
Li3Sm (mp-977286) | 0.0000 | 0.209 | 2 |
Si3Ge (mp-972751) | 0.0000 | 0.528 | 2 |
K3Sn (mp-973614) | 0.0000 | 0.105 | 2 |
Li3Ag (mp-865875) | 0.0000 | 0.000 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Y_sv Al |
Final Energy/Atom-5.0633 eV |
Corrected Energy-20.2531 eV
-20.2531 eV = -20.2531 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)