Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.401 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.43 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTmAl3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 98.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 1> | 297.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 230.7 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 200.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 171.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 143.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 164.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 230.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 230.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 164.8 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 314.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 230.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 114.5 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 178.6 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 218.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 131.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 230.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 314.9 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 286.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 297.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 263.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 286.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 297.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 296.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 247.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 178.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 314.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 314.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 230.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 114.5 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 261.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 349.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 178.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 171.8 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 347.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 257.6 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 314.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 314.9 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 349.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 305.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 33.0 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 218.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 164.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 65.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 218.3 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 286.3 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 200.4 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 218.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 263.7 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 297.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbMg6Zr (mp-1022554) | 0.3194 | 0.263 | 3 |
RbMg6Nb (mp-1017237) | 0.3226 | 0.388 | 3 |
HoGa3 (mp-982557) | 0.1212 | 0.014 | 2 |
LuAl3 (mp-973539) | 0.1030 | 0.021 | 2 |
CeAg3 (mp-862709) | 0.0829 | 0.039 | 2 |
DyAl3 (mp-864995) | 0.1558 | 0.000 | 2 |
DyGa3 (mp-865103) | 0.1557 | 0.006 | 2 |
Mn (mp-542909) | 0.6191 | 0.053 | 1 |
N2 (mp-672234) | 0.7427 | 0.000 | 1 |
W (mp-1065340) | 0.5582 | 0.491 | 1 |
Cs (mp-1012110) | 0.6580 | 0.046 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Al |
Final Energy/Atom-4.3296 eV |
Corrected Energy-34.6370 eV
-34.6370 eV = -34.6370 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)