Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.594 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTb14Ag51 + TbAg2 + Tb5Ir3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 249.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 249.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 141.3 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 86.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 349.7 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 211.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 282.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 211.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 199.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 282.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 70.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 349.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 282.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 211.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 50.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 199.8 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 249.8 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 149.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 349.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 149.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 149.9 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 349.7 |
Al (mp-134) | <1 1 0> | <1 1 0> | 70.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 249.8 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 211.9 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 282.6 |
C (mp-66) | <1 1 0> | <1 0 0> | 249.8 |
C (mp-66) | <1 1 1> | <1 0 0> | 349.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 282.6 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 173.0 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 249.8 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 349.7 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 249.8 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 149.9 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 211.9 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 211.9 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 249.8 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 249.8 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 50.0 |
Ni (mp-23) | <1 1 1> | <1 1 1> | 86.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 199.8 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 211.9 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 249.8 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 249.8 |
Si (mp-149) | <1 0 0> | <1 0 0> | 249.8 |
Au (mp-81) | <1 1 1> | <1 0 0> | 149.9 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 199.8 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 211.9 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 259.6 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 349.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
141 | 81 | 81 | 0 | 0 | 0 |
81 | 141 | 81 | 0 | 0 | 0 |
81 | 81 | 141 | 0 | 0 | 0 |
0 | 0 | 0 | 31 | 0 | 0 |
0 | 0 | 0 | 0 | 31 | 0 |
0 | 0 | 0 | 0 | 0 | 31 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
12.3 | -4.5 | -4.5 | 0 | 0 | 0 |
-4.5 | 12.3 | -4.5 | 0 | 0 | 0 |
-4.5 | -4.5 | 12.3 | 0 | 0 | 0 |
0 | 0 | 0 | 32.4 | 0 | 0 |
0 | 0 | 0 | 0 | 32.4 | 0 |
0 | 0 | 0 | 0 | 0 | 32.4 |
Shear Modulus GV30 GPa |
Bulk Modulus KV101 GPa |
Shear Modulus GR30 GPa |
Bulk Modulus KR101 GPa |
Shear Modulus GVRH30 GPa |
Bulk Modulus KVRH101 GPa |
Elastic Anisotropy0.00 |
Poisson's Ratio0.36 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiLuPt2 (mp-861652) | 0.0000 | 0.012 | 3 |
Sc2CuTc (mp-862376) | 0.0000 | 0.002 | 3 |
Er2ZnIn (mp-862788) | 0.0000 | 0.000 | 3 |
Mn2VSi (mp-865026) | 0.0000 | 0.000 | 3 |
LiHfPd2 (mp-867119) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
K3Hg (mp-983388) | 0.0000 | 0.063 | 2 |
SbPt3 (mp-973353) | 0.0000 | 0.123 | 2 |
ScZn3 (mp-973143) | 0.0000 | 0.018 | 2 |
Yb3Os (mp-980006) | 0.0000 | 0.236 | 2 |
Rb3Sn (mp-974789) | 0.0000 | 0.152 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Ag Ir |
Final Energy/Atom-5.8289 eV |
Corrected Energy-23.3155 eV
-23.3155 eV = -23.3155 eV (uncorrected energy)
|