Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.819 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.942 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 307.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 245.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 90.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 307.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 307.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 173.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 307.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 90.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 109.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 195.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 90.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 184.2 |
Al (mp-134) | <1 0 0> | <1 1 0> | 195.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 90.7 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 181.3 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 272.0 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 307.0 |
TeO2 (mp-2125) | <1 1 0> | <1 1 0> | 195.7 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 184.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 307.0 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 61.4 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 0> | 90.7 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 90.7 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 173.4 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 61.4 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 173.4 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 90.7 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 1> | 109.5 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 181.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 272.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 184.2 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 122.8 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 61.4 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 173.4 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 307.0 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 0> | 90.7 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 1> | 109.5 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 272.0 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 307.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 307.0 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 307.0 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 245.6 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 307.0 |
C (mp-48) | <1 0 0> | <0 1 0> | 272.0 |
C (mp-48) | <1 1 0> | <0 1 0> | 272.0 |
C (mp-48) | <1 1 1> | <0 1 0> | 272.0 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 307.0 |
NaCl (mp-22862) | <1 1 0> | <0 1 0> | 90.7 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 173.4 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 173.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2Ge2O5 (mp-771185) | 0.7391 | 0.008 | 3 |
Sm2V2O7 (mp-772672) | 0.6484 | 0.116 | 3 |
K15Os7N19 (mp-1029965) | 0.7106 | 0.122 | 3 |
Na15Cr7N19 (mp-1029705) | 0.7187 | 0.000 | 3 |
Na15Re7N19 (mp-1029650) | 0.7097 | 0.000 | 3 |
Li3Bi(PO4)2 (mp-778460) | 0.6089 | 0.054 | 4 |
BAs5(Pb3O10)2 (mp-622018) | 0.6887 | 0.000 | 4 |
KNaGeO3 (mp-558085) | 0.6982 | 0.000 | 4 |
CaCrAs2O7 (mvc-7968) | 0.6934 | 0.082 | 4 |
CaCuAs2O7 (mp-6203) | 0.6721 | 0.050 | 4 |
ZnAsHPbO5 (mp-510279) | 0.6560 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Li_sv Ta_pv N F |
Final Energy/Atom-7.1216 eV |
Corrected Energy-455.7853 eV
-455.7853 eV = -455.7853 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)