Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.296 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 235.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 272.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 277.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 277.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 118.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 170.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 198.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 118.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 136.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 306.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 277.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 272.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 198.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 118.9 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 118.9 |
BN (mp-984) | <1 0 0> | <1 0 1> | 156.6 |
BN (mp-984) | <1 1 0> | <1 0 1> | 261.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 158.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 170.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 277.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 136.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 158.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 238.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 198.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 118.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 136.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 294.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 170.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 313.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 340.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 198.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 277.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 277.3 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 136.0 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 294.4 |
TeO2 (mp-2125) | <1 1 0> | <1 1 1> | 283.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 118.9 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 283.9 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 212.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 306.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 306.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 158.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 136.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 158.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 1> | 156.6 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 176.7 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 102.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 238.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 277.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 306.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
77 | 48 | 38 | 0 | 0 | 0 |
48 | 77 | 38 | 0 | 0 | 0 |
38 | 38 | 109 | 0 | 0 | 0 |
0 | 0 | 0 | 25 | 0 | 0 |
0 | 0 | 0 | 0 | 25 | 0 |
0 | 0 | 0 | 0 | 0 | 14 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
22.6 | -12.4 | -3.6 | 0 | 0 | 0 |
-12.4 | 22.6 | -3.6 | 0 | 0 | 0 |
-3.6 | -3.6 | 11.7 | 0 | 0 | 0 |
0 | 0 | 0 | 40.2 | 0 | 0 |
0 | 0 | 0 | 0 | 40.2 | 0 |
0 | 0 | 0 | 0 | 0 | 70.1 |
Shear Modulus GV22 GPa |
Bulk Modulus KV57 GPa |
Shear Modulus GR20 GPa |
Bulk Modulus KR56 GPa |
Shear Modulus GVRH21 GPa |
Bulk Modulus KVRH56 GPa |
Elastic Anisotropy0.56 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.6019 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.4538 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.5486 | 0.193 | 4 |
TbCd3 (mp-30498) | 0.1094 | 0.003 | 2 |
PrHg3 (mp-861487) | 0.1097 | 0.000 | 2 |
ScZn3 (mp-862260) | 0.0885 | 0.000 | 2 |
HfZn3 (mp-866108) | 0.0672 | 0.000 | 2 |
LaHg3 (mp-862332) | 0.1030 | 0.000 | 2 |
Hg (mp-975272) | 0.4035 | 0.001 | 1 |
Cr (mp-89) | 0.4121 | 0.420 | 1 |
Tl (mp-972351) | 0.3521 | 0.000 | 1 |
Hg (mp-569360) | 0.3726 | 0.001 | 1 |
Ce (mp-20736) | 0.4234 | 0.081 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Cd |
Final Energy/Atom-2.1682 eV |
Corrected Energy-17.3457 eV
-17.3457 eV = -17.3457 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)