Final Magnetic Moment0.089 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.082 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.082 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNb + Ti |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 281.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 271.7 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 77.6 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 271.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 31.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 1> | 210.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 155.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 232.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 281.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 284.2 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 271.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 187.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 142.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 31.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 172.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 177.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 150.7 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 157.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 78.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 284.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 201.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 250.3 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 155.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 62.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 250.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 78.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 177.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 284.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 31.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 232.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 281.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 31.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 213.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 271.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 219.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 297.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 78.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 109.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 15.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 140.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 248.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 203.4 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 201.0 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 194.1 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 116.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 281.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 140.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 265.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 271.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 234.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
136 | 120 | 108 | 0 | 0 | 0 |
120 | 136 | 108 | 0 | 0 | 0 |
108 | 108 | 159 | 0 | 0 | 0 |
0 | 0 | 0 | 38 | 0 | 0 |
0 | 0 | 0 | 0 | 38 | 0 |
0 | 0 | 0 | 0 | 0 | 39 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
36.4 | -27.3 | -6.2 | 0 | 0 | 0 |
-27.3 | 36.4 | -6.2 | 0 | 0 | 0 |
-6.2 | -6.2 | 14.7 | 0 | 0 | 0 |
0 | 0 | 0 | 26.2 | 0 | 0 |
0 | 0 | 0 | 0 | 26.2 | 0 |
0 | 0 | 0 | 0 | 0 | 25.9 |
Shear Modulus GV29 GPa |
Bulk Modulus KV123 GPa |
Shear Modulus GR20 GPa |
Bulk Modulus KR122 GPa |
Shear Modulus GVRH25 GPa |
Bulk Modulus KVRH122 GPa |
Elastic Anisotropy2.27 |
Poisson's Ratio0.41 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GaCo2Ni (mp-20551) | 0.5107 | 0.080 | 3 |
MnGaFe2 (mp-1065753) | 0.5385 | 0.053 | 3 |
HfTl3 (mp-982930) | 0.0121 | 0.260 | 2 |
ScSn3 (mp-981383) | 0.0040 | 0.093 | 2 |
Lu3Si (mp-976355) | 0.0437 | 0.242 | 2 |
ZrAl3 (mp-1065309) | 0.0161 | 0.025 | 2 |
U3Cl (mp-972405) | 0.0282 | 0.820 | 2 |
Na (mp-974920) | 0.5686 | 0.002 | 1 |
Rb (mp-975519) | 0.4949 | 0.017 | 1 |
Ba (mp-1058581) | 0.4543 | 0.019 | 1 |
Cs (mp-1012110) | 0.5682 | 0.046 | 1 |
In (mp-1055994) | 0.4726 | 0.030 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv Nb_pv |
Final Energy/Atom-8.3650 eV |
Corrected Energy-33.4599 eV
-33.4599 eV = -33.4599 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)