Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.460 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.460 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density16.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToIr + Hg |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 343.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 209.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 293.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 172.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 155.2 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 83.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 207.0 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 293.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 224.2 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 108.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 207.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 310.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 170.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 310.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 283.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 191.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 155.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 34.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 241.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 86.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 241.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 152.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 167.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 138.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 155.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 34.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 241.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 17.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 69.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 86.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 114.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 162.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 172.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 310.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 120.7 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 83.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 172.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 251.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 327.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 293.2 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 125.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 17.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 120.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 86.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 86.2 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 305.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 209.5 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 267.3 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 125.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 189.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
135 | 156 | 108 | 0 | 0 | 0 |
156 | 135 | 108 | 0 | 0 | 0 |
108 | 108 | 158 | 0 | 0 | 0 |
0 | 0 | 0 | 10 | 0 | 0 |
0 | 0 | 0 | 0 | 10 | 0 |
0 | 0 | 0 | 0 | 0 | 59 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-19.6 | 26.6 | -4.8 | 0 | 0 | 0 |
26.6 | -19.6 | -4.8 | 0 | 0 | 0 |
-4.8 | -4.8 | 13 | 0 | 0 | 0 |
0 | 0 | 0 | 99.5 | 0 | 0 |
0 | 0 | 0 | 0 | 99.5 | 0 |
0 | 0 | 0 | 0 | 0 | 17 |
Shear Modulus GV19 GPa |
Bulk Modulus KV130 GPa |
Shear Modulus GR32 GPa |
Bulk Modulus KR130 GPa |
Shear Modulus GVRH25 GPa |
Bulk Modulus KVRH130 GPa |
Elastic Anisotropy-1.92 |
Poisson's Ratio0.41 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GaCo2Ni (mp-20551) | 0.3021 | 0.080 | 3 |
MnGaFe2 (mp-1065753) | 0.3299 | 0.053 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.5892 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.5968 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.6253 | 0.193 | 4 |
TaAl3 (mp-869) | 0.0261 | 0.000 | 2 |
Li3Tc (mp-977230) | 0.0074 | 0.675 | 2 |
Hg3Rh (mp-975452) | 0.0222 | 0.204 | 2 |
Be3Ir (mp-862714) | 0.0330 | 0.000 | 2 |
Al3V (mp-2554) | 0.0295 | 0.000 | 2 |
Na (mp-974920) | 0.3600 | 0.002 | 1 |
Rb (mp-975519) | 0.2864 | 0.017 | 1 |
Ba (mp-1058581) | 0.3029 | 0.019 | 1 |
Tl (mp-151) | 0.3718 | 0.010 | 1 |
In (mp-1055994) | 0.2640 | 0.030 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hg Ir |
Final Energy/Atom-1.9777 eV |
Corrected Energy-7.9108 eV
-7.9108 eV = -7.9108 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)