Final Magnetic Moment0.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.677 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLuHg + LuAu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 291.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 218.9 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 218.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 206.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 218.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 257.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 257.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 145.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 206.3 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 145.9 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 218.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 51.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 154.8 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 218.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 257.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 257.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 145.9 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 218.9 |
BN (mp-984) | <0 0 1> | <1 1 0> | 218.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 154.8 |
BN (mp-984) | <1 1 0> | <1 1 1> | 268.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 206.3 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 218.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 268.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 309.5 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 257.9 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 268.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 291.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 257.9 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 218.9 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 268.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 206.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 257.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 257.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 291.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 257.9 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 154.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 257.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 218.9 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 218.9 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 206.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 206.3 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 291.8 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 154.8 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 218.9 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 218.9 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 73.0 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 89.3 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 89.3 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 291.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
105 | 73 | 73 | 0 | 0 | 0 |
73 | 105 | 73 | 0 | 0 | 0 |
73 | 73 | 105 | 0 | 0 | 0 |
0 | 0 | 0 | 40 | 0 | 0 |
0 | 0 | 0 | 0 | 40 | 0 |
0 | 0 | 0 | 0 | 0 | 40 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
22 | -9 | -9 | 0 | 0 | 0 |
-9 | 22 | -9 | 0 | 0 | 0 |
-9 | -9 | 22 | 0 | 0 | 0 |
0 | 0 | 0 | 24.7 | 0 | 0 |
0 | 0 | 0 | 0 | 24.7 | 0 |
0 | 0 | 0 | 0 | 0 | 24.7 |
Shear Modulus GV31 GPa |
Bulk Modulus KV84 GPa |
Shear Modulus GR25 GPa |
Bulk Modulus KR84 GPa |
Shear Modulus GVRH28 GPa |
Bulk Modulus KVRH84 GPa |
Elastic Anisotropy1.09 |
Poisson's Ratio0.35 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbSmPd2 (mp-980068) | 0.0000 | 0.005 | 3 |
SmDyHg2 (mp-978557) | 0.0000 | 0.000 | 3 |
LiHf2Tc (mp-976600) | 0.0000 | 0.011 | 3 |
PaNi2Sb (mp-861992) | 0.0000 | 0.009 | 3 |
Mg2PtRh (mp-864940) | 0.0000 | 0.000 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.007 | 4 |
VGaFeCo (mp-1066581) | 0.0000 | 0.029 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
Yb3V (mp-979942) | 0.0000 | 0.458 | 2 |
Na3Ca (mp-977062) | 0.0000 | 0.085 | 2 |
SiBi3 (mp-972837) | 0.0000 | 0.434 | 2 |
NaTm3 (mp-976863) | 0.0000 | 0.326 | 2 |
Yb3U (mp-1005850) | 0.0000 | 0.627 | 2 |
Xe (mp-979285) | 0.0000 | 0.002 | 1 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Hg Au |
Final Energy/Atom-3.8321 eV |
Corrected Energy-15.3284 eV
-15.3284 eV = -15.3284 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)