Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.236 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa15Pb4 + Pd3Pb + NaPb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 78.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 226.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 226.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 127.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 255.7 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 127.8 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 319.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 191.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 234.9 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 255.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 319.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 271.2 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 319.6 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 191.8 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 255.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 255.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 191.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 234.9 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 191.8 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 191.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 180.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 191.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 255.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 226.0 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 63.9 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 78.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 226.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 226.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 45.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 226.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 191.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 255.7 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 313.2 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 319.6 |
Al (mp-134) | <1 1 0> | <1 1 0> | 255.7 |
BN (mp-984) | <0 0 1> | <1 1 1> | 234.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 226.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 255.7 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 313.2 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 63.9 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 78.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 226.0 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 255.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 90.4 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 45.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 313.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 226.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 316.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 180.8 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 45.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
41 | 32 | 32 | 0 | 0 | 0 |
32 | 41 | 32 | 0 | 0 | 0 |
32 | 32 | 41 | 0 | 0 | 0 |
0 | 0 | 0 | 24 | 0 | 0 |
0 | 0 | 0 | 0 | 24 | 0 |
0 | 0 | 0 | 0 | 0 | 24 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
76.3 | -33.4 | -33.4 | 0 | 0 | 0 |
-33.4 | 76.3 | -33.4 | 0 | 0 | 0 |
-33.4 | -33.4 | 76.3 | 0 | 0 | 0 |
0 | 0 | 0 | 41.1 | 0 | 0 |
0 | 0 | 0 | 0 | 41.1 | 0 |
0 | 0 | 0 | 0 | 0 | 41.1 |
Shear Modulus GV16 GPa |
Bulk Modulus KV35 GPa |
Shear Modulus GR9 GPa |
Bulk Modulus KR35 GPa |
Shear Modulus GVRH13 GPa |
Bulk Modulus KVRH35 GPa |
Elastic Anisotropy4.23 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KBa2Re (mp-631513) | 0.0000 | 1.271 | 3 |
BaCaRu2 (mp-631512) | 0.0000 | 0.840 | 3 |
FeTc2Cl (mp-631425) | 0.0000 | 1.059 | 3 |
HfMgRh2 (mp-865050) | 0.0000 | 0.000 | 3 |
Tm2MgIn (mp-865359) | 0.0000 | 0.000 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.007 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.163 | 4 |
K3W (mp-973446) | 0.0000 | 1.504 | 2 |
LaHg (mp-734) | 0.0000 | 0.000 | 2 |
BaZn (mp-902) | 0.0000 | 0.002 | 2 |
InRh (mp-899) | 0.0000 | 0.000 | 2 |
BeCo (mp-2773) | 0.0000 | 0.000 | 2 |
Xe (mp-979285) | 0.0000 | 0.002 | 1 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Pd Pb_d |
Final Energy/Atom-4.0826 eV |
Corrected Energy-16.3303 eV
-16.3303 eV = -16.3303 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)