Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.498 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.382 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGeO2 + Ge |
Band Gap0.753 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 24.7 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 141.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 74.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 120.9 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 123.4 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 24.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 141.0 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 181.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 80.6 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 197.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 28.5 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 40.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 256.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 128.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 181.3 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 172.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 356.1 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 161.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 156.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 85.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 213.7 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 60.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 284.9 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 296.1 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 362.6 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 313.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 161.2 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 123.4 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 60.4 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 74.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 60.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 261.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 161.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 181.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 213.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 128.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 270.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 185.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 161.2 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 322.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 128.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 181.3 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 172.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 128.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 181.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 320.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 213.7 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 342.5 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 284.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 128.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
287 | 100 | 100 | 0 | 0 | 0 |
100 | 287 | 100 | 0 | 0 | 0 |
100 | 100 | 287 | 0 | 0 | 0 |
0 | 0 | 0 | 108 | 0 | 0 |
0 | 0 | 0 | 0 | 108 | 0 |
0 | 0 | 0 | 0 | 0 | 108 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.2 | -1.1 | -1.1 | 0 | 0 | 0 |
-1.1 | 4.2 | -1.1 | 0 | 0 | 0 |
-1.1 | -1.1 | 4.2 | 0 | 0 | 0 |
0 | 0 | 0 | 9.2 | 0 | 0 |
0 | 0 | 0 | 0 | 9.2 | 0 |
0 | 0 | 0 | 0 | 0 | 9.2 |
Shear Modulus GV103 GPa |
Bulk Modulus KV162 GPa |
Shear Modulus GR102 GPa |
Bulk Modulus KR162 GPa |
Shear Modulus GVRH102 GPa |
Bulk Modulus KVRH162 GPa |
Elastic Anisotropy0.03 |
Poisson's Ratio0.24 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaSrO3 (mp-977112) | 0.0000 | 0.531 | 3 |
PuBO3 (mp-975564) | 0.0000 | 0.778 | 3 |
RbAsO3 (mp-975425) | 0.0000 | 0.201 | 3 |
YbMgO3 (mp-972160) | 0.0000 | 0.364 | 3 |
TaTlO3 (mp-861873) | 0.0000 | 0.107 | 3 |
Ba2VFeO6 (mp-1096778) | 0.0000 | 2.272 | 4 |
Ba2ScSbO6 (mp-20709) | 0.0000 | 2.196 | 4 |
Ba2YbSbO6 (mp-14223) | 0.0000 | 1.747 | 4 |
Ba2YSbO6 (mp-14226) | 0.0000 | 2.082 | 4 |
Ba2NbFeO6 (mp-1096853) | 0.0000 | 2.749 | 4 |
Ba3Sb2 (mp-1013582) | 0.0000 | 0.409 | 2 |
Fe4N (mp-535) | 0.0000 | 0.070 | 2 |
Mn4N (mp-505622) | 0.0000 | 0.000 | 2 |
Ba3P2 (mp-1013551) | 0.0000 | 0.446 | 2 |
Ba3As2 (mp-1013560) | 0.0000 | 0.418 | 2 |
BaLaMgBiO6 (mp-41414) | 0.0488 | 0.096 | 5 |
BaLaMgNbO6 (mp-39288) | 0.0712 | 0.090 | 5 |
SrLaNbZnO6 (mp-41918) | 0.0665 | 0.126 | 5 |
SrLaMnCoO6 (mp-40761) | 0.0404 | 0.247 | 5 |
Sr6Ca2MnFe7O24 (mp-1075969) | 0.0482 | 0.021 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.7380 | 0.065 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ge_d O |
Final Energy/Atom-5.8927 eV |
Corrected Energy-31.5703 eV
-31.5703 eV = -29.4634 eV (uncorrected energy) - 2.1069 eV (MP Anion Correction)
|