Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.612 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.329 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPbO2 + Au2O3 + Au |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 170.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 219.1 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 121.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 219.1 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 194.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 154.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 267.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 208.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 34.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 48.7 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 172.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 154.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 219.1 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 208.7 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 119.3 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 267.8 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 170.4 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 316.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 275.4 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 89.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 219.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 361.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 219.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 86.1 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 219.1 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 208.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 97.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 137.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 170.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 309.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 154.9 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 219.1 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 208.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 34.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 48.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 172.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 17.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 24.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 29.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 120.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 86.1 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 170.4 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 357.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 17.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 24.3 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 29.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 219.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 219.1 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 292.1 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 219.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
272 | 141 | 141 | 0 | 0 | 0 |
141 | 272 | 141 | 0 | 0 | 0 |
141 | 141 | 272 | 0 | 0 | 0 |
0 | 0 | 0 | 17 | 0 | 0 |
0 | 0 | 0 | 0 | 17 | 0 |
0 | 0 | 0 | 0 | 0 | 17 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5.7 | -1.9 | -1.9 | 0 | 0 | 0 |
-1.9 | 5.7 | -1.9 | 0 | 0 | 0 |
-1.9 | -1.9 | 5.7 | 0 | 0 | 0 |
0 | 0 | 0 | 58.4 | 0 | 0 |
0 | 0 | 0 | 0 | 58.4 | 0 |
0 | 0 | 0 | 0 | 0 | 58.4 |
Shear Modulus GV36 GPa |
Bulk Modulus KV184 GPa |
Shear Modulus GR24 GPa |
Bulk Modulus KR184 GPa |
Shear Modulus GVRH30 GPa |
Bulk Modulus KVRH184 GPa |
Elastic Anisotropy2.51 |
Poisson's Ratio0.42 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KTcO3 (mp-973267) | 0.0000 | 0.000 | 3 |
HfBRh3 (mp-1017578) | 0.0000 | 0.000 | 3 |
SrRhO3 (mp-1017441) | 0.0000 | 0.091 | 3 |
LaCrO3 (mp-1076719) | 0.0000 | 0.091 | 3 |
Sm3GaC (mp-10602) | 0.0000 | 0.023 | 3 |
Ba2VFeO6 (mp-1096778) | 0.0000 | 2.272 | 4 |
Ba2ScSbO6 (mp-20709) | 0.0000 | 2.196 | 4 |
Ba2YbSbO6 (mp-14223) | 0.0000 | 1.747 | 4 |
Ba2YSbO6 (mp-14226) | 0.0000 | 2.082 | 4 |
Ba2NbFeO6 (mp-1096853) | 0.0000 | 2.945 | 4 |
Fe4N (mp-535) | 0.0000 | 0.070 | 2 |
Ni4N (mp-20839) | 0.0000 | 2.019 | 2 |
Ba3Bi2 (mp-1013736) | 0.0000 | 0.388 | 2 |
Sr3As2 (mp-1013559) | 0.0000 | 0.367 | 2 |
Ba3As2 (mp-1013560) | 0.0000 | 0.418 | 2 |
BaLaMgBiO6 (mp-41414) | 0.0488 | 0.096 | 5 |
BaLaMgNbO6 (mp-39288) | 0.0712 | 0.090 | 5 |
SrLaNbZnO6 (mp-41918) | 0.0665 | 0.126 | 5 |
SrLaMnCoO6 (mp-40761) | 0.0404 | 0.249 | 5 |
Sr6Ca2MnFe7O24 (mp-1075969) | 0.0482 | 0.021 | 5 |
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) | 0.7380 | 0.065 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pb_d Au O |
Final Energy/Atom-4.5568 eV |
Corrected Energy-24.8909 eV
-24.8909 eV = -22.7840 eV (uncorrected energy) - 2.1069 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)