Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.814 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.814 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYb + W |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 254.9 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 109.3 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 254.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 291.4 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 182.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 164.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 1> | 226.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 164.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 275.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 288.5 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 189.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 145.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 288.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 315.4 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 226.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 327.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 182.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 288.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 252.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 288.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 275.0 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 226.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 275.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 164.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 275.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 275.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 288.5 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 327.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 145.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 247.3 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 315.4 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 150.7 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 275.0 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 226.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 109.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 189.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 288.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 291.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 288.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 206.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 254.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 123.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 123.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 164.9 |
BN (mp-984) | <0 0 1> | <1 1 0> | 315.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 291.4 |
BN (mp-984) | <1 0 1> | <1 0 0> | 254.9 |
BN (mp-984) | <1 1 0> | <1 1 1> | 301.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 164.9 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 72.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbMg6Zr (mp-1022554) | 0.2253 | 0.263 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.7232 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.6015 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.6569 | 0.193 | 4 |
Sm3Zn (mp-982044) | 0.1048 | 0.120 | 2 |
Tb3Si (mp-972310) | 0.0905 | 0.198 | 2 |
K3Co (mp-976583) | 0.0864 | 0.937 | 2 |
Pr3Al (mp-1079266) | 0.0453 | 0.024 | 2 |
Nd3Al (mp-1080098) | 0.0795 | 0.021 | 2 |
Hg (mp-975272) | 0.5148 | 0.001 | 1 |
Tl (mp-972351) | 0.5065 | 0.000 | 1 |
Hg (mp-569360) | 0.4682 | 0.001 | 1 |
W (mp-1065340) | 0.4762 | 0.491 | 1 |
Cs (mp-1012110) | 0.4794 | 0.046 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 W_pv |
Final Energy/Atom-3.5807 eV |
Corrected Energy-28.6457 eV
-28.6457 eV = -28.6457 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)