Final Magnetic Moment3.502 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom1.295 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.295 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa + Re |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 278.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 289.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 236.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 278.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 236.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 314.6 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 157.3 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 289.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 278.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 278.1 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 278.1 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 236.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 222.5 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 236.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 278.1 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 236.0 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 289.0 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 314.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 166.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 289.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 333.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 236.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 157.3 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 333.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 157.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 222.5 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 236.0 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 289.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 157.3 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 289.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 222.5 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 236.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 96.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 278.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 314.6 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 236.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 222.5 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 236.0 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 289.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 278.1 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 314.6 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 278.1 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 1> | 289.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 111.2 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 314.6 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 236.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 278.1 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 289.0 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 166.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 278.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
21 | 27 | 27 | 0 | 0 | 0 |
27 | 21 | 27 | 0 | 0 | 0 |
27 | 27 | 21 | 0 | 0 | 0 |
0 | 0 | 0 | 14 | 0 | 0 |
0 | 0 | 0 | 0 | 14 | 0 |
0 | 0 | 0 | 0 | 0 | 14 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-95.4 | 54.3 | 54.3 | 0 | 0 | 0 |
54.3 | -95.4 | 54.3 | 0 | 0 | 0 |
54.3 | 54.3 | -95.4 | 0 | 0 | 0 |
0 | 0 | 0 | 71.8 | 0 | 0 |
0 | 0 | 0 | 0 | 71.8 | 0 |
0 | 0 | 0 | 0 | 0 | 71.8 |
Shear Modulus GV7 GPa |
Bulk Modulus KV25 GPa |
Shear Modulus GR-13 GPa |
Bulk Modulus KR25 GPa |
Shear Modulus GVRH-3 GPa |
Bulk Modulus KVRH25 GPa |
Elastic Anisotropy-7.69 |
Poisson's Ratio0.56 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiTmAu2 (mp-861664) | 0.0000 | 0.005 | 3 |
Sc2TlCd (mp-861918) | 0.0000 | 0.000 | 3 |
LiTaRh2 (mp-861951) | 0.0000 | 0.000 | 3 |
HfZnNi2 (mp-864807) | 0.0000 | 0.000 | 3 |
Li2DyTl (mp-865581) | 0.0000 | 0.000 | 3 |
TiGaFeCo (mp-998964) | 0.0000 | 0.000 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.344 | 4 |
MnGaFeCo (mp-999552) | 0.0000 | 0.044 | 4 |
RbCa3 (mp-975390) | 0.0000 | 0.227 | 2 |
Rb3Os (mp-974843) | 0.0000 | 1.410 | 2 |
RePb3 (mp-974611) | 0.0000 | 1.029 | 2 |
Li3Tc (mp-976334) | 0.0000 | 0.614 | 2 |
Li3Ga (mp-976023) | 0.0000 | 0.013 | 2 |
Xe (mp-979285) | 0.0000 | 0.002 | 1 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Re_pv |
Final Energy/Atom-2.7999 eV |
Corrected Energy-11.1996 eV
-11.1996 eV = -11.1996 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)