Final Magnetic Moment0.034 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.798 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.006 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 151.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 151.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 151.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 151.5 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 151.5 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 151.5 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 151.5 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 151.5 |
Si (mp-149) | <1 0 0> | <1 0 0> | 151.5 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 151.5 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 151.5 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 151.5 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 151.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Th6Mg23 (mp-570442) | 0.6203 | 0.003 | 2 |
Th6Mn23 (mp-31222) | 0.6903 | 0.050 | 2 |
Er6Zn23 (mp-30615) | 0.6211 | 0.000 | 2 |
Zr6Fe23 (mp-582924) | 0.7042 | 0.007 | 2 |
Sr6Li23 (mp-2272) | 0.7193 | 0.002 | 2 |
Mn6Ni16As7 (mp-21628) | 0.1511 | 0.000 | 3 |
V6Si7Ni16 (mp-636953) | 0.2490 | 0.007 | 3 |
Cr6Si7Ni16 (mp-541940) | 0.2430 | 0.077 | 3 |
Ti6Al16Ni7 (mp-865235) | 0.1016 | 0.000 | 3 |
Mn6Ni16P7 (mp-22372) | 0.2163 | 0.002 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points10 |
U Values-- |
PseudopotentialsVASP PAW: Hf_pv Al Rh_pv |
Final Energy/Atom-6.6996 eV |
Corrected Energy-194.2877 eV
-194.2877 eV = -194.2877 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)