Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.508 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.745 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 244.1 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 301.4 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 226.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 97.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 287.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 244.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 301.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 287.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 146.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 229.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 244.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 301.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 195.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 97.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 229.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 48.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 114.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 244.1 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 185.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 341.7 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 229.6 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 287.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 229.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 226.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 97.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 229.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 182.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 48.8 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 97.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 146.5 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 287.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 48.8 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 114.8 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 185.0 |
C (mp-66) | <1 1 0> | <0 1 0> | 287.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 229.6 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 244.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 175.9 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 182.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 287.0 |
LaF3 (mp-905) | <0 0 1> | <1 0 1> | 182.5 |
LaF3 (mp-905) | <1 0 1> | <0 1 0> | 287.0 |
LaF3 (mp-905) | <1 1 0> | <1 0 1> | 182.5 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 146.5 |
BN (mp-984) | <0 0 1> | <1 1 1> | 191.3 |
BN (mp-984) | <1 0 1> | <0 1 1> | 301.4 |
BN (mp-984) | <1 1 0> | <0 1 0> | 229.6 |
BN (mp-984) | <1 1 1> | <0 1 0> | 229.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 146.5 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 229.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba(ScTe2)2 (mp-17501) | 0.1449 | 0.000 | 3 |
Sr(ScS2)2 (mp-17678) | 0.1300 | 0.000 | 3 |
Ba(YS2)2 (mp-29036) | 0.0972 | 0.000 | 3 |
CaCr2O4 (mvc-11432) | 0.1392 | 0.005 | 3 |
Ca(FeO2)2 (mp-25690) | 0.1472 | 0.018 | 3 |
Ca5Sc2(CoO6)2 (mvc-13126) | 0.6781 | 0.027 | 4 |
Na3Mn4(TeO6)2 (mp-565229) | 0.5995 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Lu_3 S |
Final Energy/Atom-6.0587 eV |
Corrected Energy-180.2584 eV
-180.2584 eV = -169.6431 eV (uncorrected energy) - 10.6154 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)