Final Magnetic Moment0.308 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom1.476 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom1.476 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa + Re |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 313.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 362.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 151.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 265.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 188.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 265.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 36.2 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 157.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 144.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 108.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 144.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 62.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 108.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 188.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 220.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 265.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 188.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 113.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 144.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 217.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 113.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 220.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 217.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 265.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 189.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 37.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 253.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 72.5 |
BN (mp-984) | <1 0 1> | <1 0 1> | 262.3 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 253.6 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 188.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 265.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 108.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 181.1 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 125.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 326.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 181.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 151.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 113.8 |
Al (mp-134) | <1 1 0> | <1 1 0> | 188.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 108.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 217.4 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 1> | 220.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 217.4 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 262.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 265.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 188.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 189.7 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 181.1 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 72.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr8Ni50Mo15W2 (mp-767372) | 0.3162 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.1994 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.3190 | 0.193 | 4 |
NaLi3 (mp-973316) | 0.0933 | 0.047 | 2 |
Li3Co (mp-977165) | 0.0497 | 0.366 | 2 |
Li3Be (mp-977119) | 0.0309 | 0.245 | 2 |
Rb3Er (mp-974672) | 0.0905 | 0.631 | 2 |
Rb3Pr (mp-974662) | 0.0859 | 0.580 | 2 |
Y (mp-1059189) | 0.2340 | 0.003 | 1 |
Er (mp-99) | 0.2483 | 0.010 | 1 |
Dy (mp-88) | 0.2493 | 0.019 | 1 |
Ho (mp-144) | 0.2483 | 0.014 | 1 |
Tm (mp-143) | 0.2488 | 0.003 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Re_pv |
Final Energy/Atom-2.6189 eV |
Corrected Energy-20.9510 eV
-20.9510 eV = -20.9510 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)