Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.197 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.387 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.25 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Au2O3 + Au
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdTe (mp-406) <1 0 0> <1 1 1> 0.003 306.5
InSb (mp-20012) <1 0 0> <1 1 1> 0.006 306.5
TiO2 (mp-2657) <1 0 1> <1 1 1> 0.007 306.5
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.010 183.9
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.011 328.4
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.013 240.9
MgF2 (mp-1249) <0 0 1> <1 1 1> 0.013 306.5
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.016 240.8
AlN (mp-661) <0 0 1> <1 0 0> 0.016 153.2
Ga2O3 (mp-886) <1 1 0> <1 0 0> 0.018 218.9
Mg (mp-153) <1 0 1> <1 0 0> 0.020 284.6
MoSe2 (mp-1634) <1 0 1> <1 0 0> 0.022 262.7
Te2W (mp-22693) <0 0 1> <1 1 1> 0.023 245.2
LaAlO3 (mp-2920) <1 1 0> <1 1 1> 0.024 122.6
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.025 109.5
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.026 341.2
C (mp-48) <0 0 1> <1 1 0> 0.027 189.6
Au (mp-81) <1 0 0> <1 0 0> 0.032 87.6
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.032 306.5
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.039 284.6
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.039 218.9
C (mp-66) <1 0 0> <1 0 0> 0.040 218.9
C (mp-48) <1 1 1> <1 1 1> 0.041 306.5
GaN (mp-804) <0 0 1> <0 0 1> 0.041 144.5
BaTiO3 (mp-5986) <0 0 1> <1 1 0> 0.042 303.3
SiC (mp-11714) <1 0 1> <1 1 0> 0.046 227.5
BN (mp-984) <1 0 1> <1 0 0> 0.048 240.8
MgF2 (mp-1249) <1 0 0> <1 1 0> 0.049 303.3
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.055 197.0
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.055 109.5
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.057 197.0
C (mp-66) <1 1 0> <1 0 0> 0.060 197.0
TiO2 (mp-390) <0 0 1> <0 0 1> 0.063 144.5
C (mp-48) <1 0 0> <1 0 0> 0.071 175.1
InP (mp-20351) <1 1 0> <1 1 0> 0.074 151.7
TePb (mp-19717) <1 1 0> <0 0 1> 0.077 240.9
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.079 189.6
Ag (mp-124) <1 0 0> <1 0 0> 0.079 87.6
SiC (mp-11714) <1 0 0> <1 0 0> 0.084 218.9
Ge (mp-32) <1 1 0> <1 0 0> 0.095 284.6
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.097 109.5
CeO2 (mp-20194) <1 1 1> <1 1 1> 0.099 306.5
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.103 265.4
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.104 303.3
BN (mp-984) <1 0 0> <1 0 0> 0.104 175.1
Si (mp-149) <1 1 1> <1 1 1> 0.106 306.5
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.107 328.4
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.108 189.6
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.111 144.5
YAlO3 (mp-3792) <0 1 1> <1 0 0> 0.111 284.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
118 105 112 0 0 0
105 118 112 0 0 0
112 112 185 0 0 0
0 0 0 -2 0 0
0 0 0 0 -2 0
0 0 0 0 0 7
Compliance Tensor Sij (10-12Pa-1)
44 -32.6 -6.9 0 0 0
-32.6 44 -6.9 0 0 0
-6.9 -6.9 13.8 0 0 0
0 0 0 -518.4 0 0
0 0 0 0 -518.4 0
0 0 0 0 0 153.1
Shear Modulus GV
7 GPa
Bulk Modulus KV
120 GPa
Shear Modulus GR
-7 GPa
Bulk Modulus KR
112 GPa
Shear Modulus GVRH
-0 GPa
Bulk Modulus KVRH
116 GPa
Elastic Anisotropy
-9.51
Poisson's Ratio
0.50

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiMoS2 (mp-30248) 0.7343 0.023 3
Rb2ZrTe3 (mp-29603) 0.7026 0.000 3
Pa3H (mp-982244) 0.5595 0.665 2
CrAs (mp-20717) 0.5865 0.000 2
CrAs (mp-1078213) 0.5861 0.000 2
BPt3 (mp-861943) 0.3769 0.113 2
TiSe (mp-571651) 0.5660 0.013 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Au O
Final Energy/Atom
-3.3241 eV
Corrected Energy
-27.9669 eV
Uncorrected energy = -26.5929 eV Composition-based energy adjustment (-0.687 eV/atom x 2.0 atoms) = -1.3740 eV Corrected energy = -27.9669 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)