Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.550 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.189 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 294.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 286.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 147.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 220.9 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 294.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 220.9 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 161.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 147.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 206.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 143.3 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 286.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 294.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 286.6 |
Al (mp-134) | <1 1 0> | <1 0 1> | 206.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 220.9 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 294.5 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 143.3 |
TeO2 (mp-2125) | <1 0 1> | <0 1 1> | 160.2 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 143.3 |
C (mp-66) | <1 1 1> | <1 0 0> | 220.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 214.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 73.6 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 103.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 294.5 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 147.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 147.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 147.2 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 294.5 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 147.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 220.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 294.5 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 286.6 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 214.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 286.6 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 1> | 206.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 220.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 147.2 |
Si (mp-149) | <1 0 0> | <1 0 0> | 147.2 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 206.9 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 286.6 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 214.9 |
C (mp-48) | <1 0 0> | <0 0 1> | 286.6 |
C (mp-48) | <1 0 1> | <1 0 0> | 220.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 71.6 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 103.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 220.9 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 294.5 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 286.6 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 143.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 286.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaAsS2 (mp-5942) | 0.4002 | 0.000 | 3 |
NaAsSe2 (mp-27374) | 0.3511 | 0.002 | 3 |
Na2TeSe3 (mp-573581) | 0.4916 | 0.000 | 3 |
LiAsS2 (mp-555874) | 0.4563 | 0.000 | 3 |
K2TeSe3 (mp-28419) | 0.5164 | 0.000 | 3 |
Li2VO2F (mp-763225) | 0.6209 | 0.103 | 4 |
Li2VO2F (mp-763190) | 0.7071 | 0.217 | 4 |
Na3LiMn5O9 (mp-762649) | 0.6959 | 0.338 | 4 |
Li2VO2F (mp-763193) | 0.7079 | 0.204 | 4 |
Na3Cu2SbO6 (mp-12860) | 0.6944 | 0.056 | 4 |
Te2Au (mp-20123) | 0.6667 | 0.000 | 2 |
NaLiV(OF)2 (mp-764851) | 0.7426 | 0.078 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv As Se |
Final Energy/Atom-3.7907 eV |
Corrected Energy-128.8533 eV
Uncorrected energy = -121.3013 eV
Composition-based energy adjustment (-0.472 eV/atom x 16.0 atoms) = -7.5520 eV
Corrected energy = -128.8533 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)