Final Magnetic Moment0.037 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.975 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.975 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToN2 + Ag |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 77.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 215.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 77.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 77.1 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 315.6 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 190.6 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 135.2 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 142.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 30.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 127.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 154.2 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 135.2 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 95.6 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 223.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 77.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 283.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 255.0 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 177.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 283.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 190.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 246.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 200.5 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 177.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 169.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 169.6 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 247.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 45.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 231.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 61.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 246.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 223.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 15.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 45.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 1> | 95.3 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 238.2 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 225.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 270.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 95.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 293.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 77.1 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 135.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 200.5 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 135.2 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 95.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 138.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 283.3 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 247.9 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 177.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 95.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 231.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
26 | 211 | 89 | 0 | 0 | 0 |
211 | 26 | 89 | 0 | 0 | 0 |
89 | 89 | 116 | 0 | 0 | 0 |
0 | 0 | 0 | 15 | 0 | 0 |
0 | 0 | 0 | 0 | 15 | 0 |
0 | 0 | 0 | 0 | 0 | 38 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
2.3 | 7.7 | -7.7 | 0 | 0 | 0 |
7.7 | 2.3 | -7.7 | 0 | 0 | 0 |
-7.7 | -7.7 | 20.5 | 0 | 0 | 0 |
0 | 0 | 0 | 65.6 | 0 | 0 |
0 | 0 | 0 | 0 | 65.6 | 0 |
0 | 0 | 0 | 0 | 0 | 26.2 |
Shear Modulus GV-1 GPa |
Bulk Modulus KV105 GPa |
Shear Modulus GR25 GPa |
Bulk Modulus KR103 GPa |
Shear Modulus GVRH12 GPa |
Bulk Modulus KVRH104 GPa |
Elastic Anisotropy-5.20 |
Poisson's Ratio0.45 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.0449 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.1381 | 0.034 | 3 |
LiCa6Ge (mp-12609) | 0.1573 | 0.183 | 3 |
GaFeNi2 (mp-1065359) | 0.1401 | 0.065 | 3 |
GaCo2Ni (mp-1018060) | 0.1499 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.1799 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3150 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3625 | 0.193 | 4 |
KNd3 (mp-982195) | 0.0041 | 0.447 | 2 |
Sm3Cr (mp-978825) | 0.0107 | 0.359 | 2 |
Pr3Cd (mp-975641) | 0.0093 | 0.056 | 2 |
Zn3C (mp-981336) | 0.0076 | 1.046 | 2 |
NbNi3 (mp-11513) | 0.0024 | 0.008 | 2 |
In (mp-85) | 0.0838 | 0.037 | 1 |
Pr (mp-97) | 0.1383 | 0.008 | 1 |
Ce (mp-567332) | 0.1320 | 0.000 | 1 |
Rb (mp-12628) | 0.1310 | 0.015 | 1 |
La (mp-156) | 0.0491 | 0.001 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag N |
Final Energy/Atom-3.1377 eV |
Corrected Energy-12.5508 eV
-12.5508 eV = -12.5508 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)