Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.876 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 224.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 224.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 123.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 155.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 142.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 259.5 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 222.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 224.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 328.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 207.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 51.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 224.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 121.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 207.6 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 311.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 276.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 164.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 69.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 222.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 164.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 346.0 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 284.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 69.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 246.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 207.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 287.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 69.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 222.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 213.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 276.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 69.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 311.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 164.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 224.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 82.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 246.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 207.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 284.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 207.6 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 267.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 121.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 82.1 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 311.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 328.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 276.8 |
Te2W (mp-22693) | <1 0 0> | <1 1 1> | 292.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 123.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 224.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 164.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 276.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
115 | 38 | 34 | 0 | 0 | 0 |
38 | 115 | 34 | 0 | 0 | 0 |
34 | 34 | 78 | 0 | 0 | 0 |
0 | 0 | 0 | 29 | 0 | 0 |
0 | 0 | 0 | 0 | 29 | 0 |
0 | 0 | 0 | 0 | 0 | 38 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
10.6 | -2.5 | -3.6 | 0 | 0 | 0 |
-2.5 | 10.6 | -3.6 | 0 | 0 | 0 |
-3.6 | -3.6 | 16 | 0 | 0 | 0 |
0 | 0 | 0 | 34.5 | 0 | 0 |
0 | 0 | 0 | 0 | 34.5 | 0 |
0 | 0 | 0 | 0 | 0 | 26.2 |
Shear Modulus GV33 GPa |
Bulk Modulus KV58 GPa |
Shear Modulus GR32 GPa |
Bulk Modulus KR56 GPa |
Shear Modulus GVRH32 GPa |
Bulk Modulus KVRH57 GPa |
Elastic Anisotropy0.18 |
Poisson's Ratio0.26 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YHSe (mp-28797) | 0.0317 | 0.000 | 3 |
HoHSe (mp-24012) | 0.0316 | 0.000 | 3 |
BaCuSb (mp-11700) | 0.0292 | 0.000 | 3 |
BaLiP (mp-10615) | 0.0246 | 0.033 | 3 |
SrCuP (mp-16321) | 0.0133 | 0.000 | 3 |
CaGa2 (mp-992) | 0.0246 | 0.036 | 2 |
CrB2 (mp-1061685) | 0.0139 | 0.067 | 2 |
CrB2 (mp-374) | 0.0095 | 0.067 | 2 |
YbSi2 (mp-1671) | 0.0246 | 0.069 | 2 |
LaGa2 (mp-19839) | 0.0049 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv P Au |
Final Energy/Atom-4.4112 eV |
Corrected Energy-26.4671 eV
-26.4671 eV = -26.4671 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)