Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.444 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <1 0 0> | 321.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 257.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 273.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 128.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 64.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 193.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 321.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 64.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 111.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 321.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 321.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 321.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 64.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 91.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 321.8 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 321.8 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 182.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 91.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 257.4 |
BN (mp-984) | <1 0 1> | <1 1 0> | 182.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 321.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 91.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 64.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 91.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 257.4 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 182.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 64.4 |
Al (mp-134) | <1 1 1> | <1 1 1> | 111.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 128.7 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 182.0 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 273.1 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 321.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 273.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 193.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 321.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 321.8 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 273.1 |
Al (mp-134) | <1 1 0> | <1 1 0> | 91.0 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 273.1 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 193.1 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 321.8 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 64.4 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 182.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 321.8 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 128.7 |
C (mp-66) | <1 0 0> | <1 0 0> | 64.4 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 91.0 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 91.0 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 321.8 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 64.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
44 | 44 | 44 | 0 | 0 | 0 |
44 | 44 | 44 | 0 | 0 | 0 |
44 | 44 | 44 | 0 | 0 | 0 |
0 | 0 | 0 | 24 | 0 | 0 |
0 | 0 | 0 | 0 | 24 | 0 |
0 | 0 | 0 | 0 | 0 | 24 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5793.8 | -2893.2 | -2893.1 | 0 | 0 | 0 |
-2893.2 | 5793.8 | -2893.1 | 0 | 0 | 0 |
-2893.1 | -2893.1 | 5793.8 | 0 | 0 | 0 |
0 | 0 | 0 | 41.6 | 0 | 0 |
0 | 0 | 0 | 0 | 41.6 | 0 |
0 | 0 | 0 | 0 | 0 | 41.6 |
Shear Modulus GV14 GPa |
Bulk Modulus KV44 GPa |
Shear Modulus GR0 GPa |
Bulk Modulus KR44 GPa |
Shear Modulus GVRH7 GPa |
Bulk Modulus KVRH44 GPa |
Elastic Anisotropy499.12 |
Poisson's Ratio0.42 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pm2InHg (mp-982613) | 0.0000 | 0.000 | 3 |
ZnFeRh2 (mp-977361) | 0.0000 | 0.000 | 3 |
Zn2RhAu (mp-864844) | 0.0000 | 0.000 | 3 |
Yb2AgBi (mp-865546) | 0.0000 | 0.000 | 3 |
DyNbRu2 (mp-866126) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
AlNi3 (mp-672232) | 0.0000 | 0.047 | 2 |
Mn3Al (mp-973149) | 0.0000 | 0.069 | 2 |
NdAu3 (mp-975073) | 0.0000 | 0.043 | 2 |
Mo3H (mp-975814) | 0.0000 | 0.852 | 2 |
LaCd3 (mp-862559) | 0.0000 | 0.000 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Ac In_d |
Final Energy/Atom-3.3511 eV |
Corrected Energy-13.4046 eV
-13.4046 eV = -13.4046 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)