Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.075 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
BN (mp-984) | <1 0 0> | <0 1 0> | 0.003 | 115.9 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 1> | 0.006 | 179.9 |
SrTiO3 (mp-4651) | <1 1 0> | <0 1 1> | 0.008 | 249.2 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 0.009 | 162.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 0.014 | 132.4 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 0.015 | 132.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 0.015 | 88.2 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 0.016 | 44.1 |
ZnTe (mp-2176) | <1 1 0> | <1 0 0> | 0.016 | 162.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 0.017 | 162.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 0.019 | 44.1 |
SrTiO3 (mp-4651) | <0 0 1> | <0 1 1> | 0.024 | 249.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 0.031 | 308.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 0.031 | 139.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 0.031 | 347.7 |
Si (mp-149) | <1 1 1> | <0 0 1> | 0.034 | 308.8 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 0.038 | 249.2 |
CsI (mp-614603) | <1 0 0> | <0 1 1> | 0.048 | 249.2 |
ZnO (mp-2133) | <1 0 0> | <0 1 1> | 0.051 | 299.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 0.058 | 239.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 0.059 | 44.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 0.061 | 199.4 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 0.062 | 132.4 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 1> | 0.062 | 321.4 |
BN (mp-984) | <1 0 1> | <0 1 0> | 0.065 | 162.3 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 0.066 | 162.4 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 0.067 | 132.4 |
WS2 (mp-224) | <1 0 1> | <1 0 0> | 0.073 | 324.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 0.081 | 44.1 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 0.086 | 203.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 0.087 | 185.4 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 0.088 | 49.8 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 0.090 | 132.4 |
GaSb (mp-1156) | <1 1 0> | <1 0 0> | 0.090 | 162.4 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 0.100 | 92.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 0> | 0.102 | 301.3 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 0> | 0.107 | 243.6 |
Mg (mp-153) | <0 0 1> | <1 1 0> | 0.107 | 140.3 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 1> | 0.111 | 192.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 0.112 | 162.4 |
SiC (mp-8062) | <1 1 1> | <1 0 1> | 0.113 | 299.8 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 0.113 | 132.4 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 0.114 | 132.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 0.119 | 203.0 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 0.124 | 69.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 1> | 0.126 | 192.9 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 0.126 | 132.4 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 0.128 | 162.4 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 0.128 | 140.3 |
WS2 (mp-224) | <0 0 1> | <1 1 0> | 0.128 | 140.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
115 | 80 | 64 | 0 | 0 | 0 |
80 | 131 | 77 | 0 | 0 | 0 |
64 | 77 | 164 | 0 | 0 | 0 |
0 | 0 | 0 | 35 | 0 | 0 |
0 | 0 | 0 | 0 | 29 | 0 |
0 | 0 | 0 | 0 | 0 | 25 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
15.6 | -8.3 | -2.2 | 0 | 0 | 0 |
-8.3 | 15 | -3.9 | 0 | 0 | 0 |
-2.2 | -3.9 | 8.8 | 0 | 0 | 0 |
0 | 0 | 0 | 28.2 | 0 | 0 |
0 | 0 | 0 | 0 | 34.3 | 0 |
0 | 0 | 0 | 0 | 0 | 39.8 |
Shear Modulus GV31 GPa |
Bulk Modulus KV95 GPa |
Shear Modulus GR29 GPa |
Bulk Modulus KR93 GPa |
Shear Modulus GVRH30 GPa |
Bulk Modulus KVRH94 GPa |
Elastic Anisotropy0.33 |
Poisson's Ratio0.36 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaCeMg6 (mp-1099118) | 0.2087 | 0.149 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.5286 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3769 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.4950 | 0.193 | 4 |
UHg3 (mp-1079421) | 0.1475 | 0.329 | 2 |
ZrAu3 (mp-1079681) | 0.1585 | 0.000 | 2 |
MgTi2 (mp-1094381) | 0.1745 | 0.155 | 2 |
MgZn2 (mp-1094456) | 0.1758 | 0.123 | 2 |
Mg2Bi (mp-1039242) | 0.1729 | 0.163 | 2 |
Hg (mp-975272) | 0.3003 | 0.001 | 1 |
Tl (mp-972351) | 0.3331 | 0.000 | 1 |
Hg (mp-569360) | 0.2825 | 0.001 | 1 |
Eu (mp-1057315) | 0.3413 | 0.000 | 1 |
Pr (mp-1009594) | 0.3487 | 0.032 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Al Ag |
Final Energy/Atom-3.2124 eV |
Corrected Energy-19.2742 eV
-19.2742 eV = -19.2742 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)