material

Si3N4

ID:

mp-988

DOI:

10.17188/1316765


Tags: Silicon nitride - beta Silicon nitride (3/4)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.314 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.13 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
4.258 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/m [176]
Hall
-P 6c
Point Group
6/m
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 16818 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.004 152.5
BN (mp-984) <0 0 1> <0 0 1> 0.015 152.5
YVO4 (mp-19133) <1 0 0> <1 0 1> 0.029 277.7
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.034 246.5
YVO4 (mp-19133) <1 0 1> <1 0 1> 0.040 277.7
GaSe (mp-1943) <0 0 1> <0 0 1> 0.041 50.8
GaSe (mp-1943) <1 0 1> <1 0 1> 0.047 277.7
Ag (mp-124) <1 1 1> <1 0 0> 0.056 89.6
Ag (mp-124) <1 0 0> <1 1 0> 0.056 155.2
DyScO3 (mp-31120) <0 1 0> <1 1 0> 0.063 349.3
BN (mp-984) <1 0 0> <1 0 0> 0.067 134.4
Fe2O3 (mp-24972) <1 0 1> <1 0 1> 0.071 222.2
Te2W (mp-22693) <0 1 0> <1 0 0> 0.074 268.9
PbSe (mp-2201) <1 1 1> <0 0 1> 0.076 203.3
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.080 203.3
InAs (mp-20305) <1 1 0> <1 0 0> 0.104 268.9
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.104 89.6
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.113 268.9
GaSb (mp-1156) <1 1 1> <0 0 1> 0.124 203.3
SiC (mp-8062) <1 1 0> <1 0 0> 0.124 246.5
Au (mp-81) <1 1 1> <1 0 0> 0.125 89.6
Au (mp-81) <1 0 0> <1 1 0> 0.125 155.2
BN (mp-984) <1 1 0> <1 0 0> 0.132 67.2
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.138 358.5
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.140 203.3
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.143 50.8
Cu (mp-30) <1 1 0> <1 0 0> 0.154 201.7
SiO2 (mp-6930) <1 1 0> <1 0 0> 0.165 336.1
CdSe (mp-2691) <1 1 1> <0 0 1> 0.171 203.3
LaF3 (mp-905) <1 0 1> <1 0 1> 0.188 277.7
TiO2 (mp-2657) <1 1 1> <1 1 0> 0.212 116.4
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.219 152.5
C (mp-66) <1 1 0> <1 0 0> 0.222 201.7
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.238 232.9
AlN (mp-661) <1 1 1> <1 1 0> 0.251 310.5
C (mp-66) <1 1 1> <0 0 1> 0.253 152.5
TiO2 (mp-390) <0 0 1> <1 0 0> 0.256 201.7
NdGaO3 (mp-3196) <0 1 0> <1 1 1> 0.257 127.9
TeO2 (mp-2125) <1 1 0> <1 1 0> 0.266 194.1
CdSe (mp-2691) <1 1 0> <1 0 0> 0.273 268.9
C (mp-48) <1 1 1> <1 0 1> 0.283 166.6
Mg (mp-153) <1 1 0> <1 0 0> 0.310 291.3
ZrO2 (mp-2858) <1 1 -1> <1 0 1> 0.319 277.7
Al (mp-134) <1 1 0> <1 1 1> 0.321 255.8
Si (mp-149) <1 1 0> <1 1 1> 0.321 127.9
CeO2 (mp-20194) <1 1 0> <1 1 1> 0.327 127.9
GaSb (mp-1156) <1 1 0> <1 0 0> 0.330 268.9
GaP (mp-2490) <1 1 0> <1 1 1> 0.332 127.9
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.343 50.8
AlN (mp-661) <1 0 1> <1 1 0> 0.347 271.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
403 180 105 0 0 0
180 403 105 0 0 0
105 105 526 0 0 0
0 0 0 99 0 0
0 0 0 0 99 0
0 0 0 0 0 112
Compliance Tensor Sij (10-12Pa-1)
3.2 -1.3 -0.4 0 0 0
-1.3 3.2 -0.4 0 0 0
-0.4 -0.4 2 0 0 0
0 0 0 10.1 0 0
0 0 0 0 10.1 0
0 0 0 0 0 9
Shear Modulus GV
125 GPa
Bulk Modulus KV
235 GPa
Shear Modulus GR
116 GPa
Bulk Modulus KR
234 GPa
Shear Modulus GVRH
120 GPa
Bulk Modulus KVRH
234 GPa
Elastic Anisotropy
0.38
Poisson's Ratio
0.28

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.24 -0.00 0.00
-0.00 4.24 0.00
0.00 0.00 4.32
Dielectric Tensor εij (total)
8.17 -0.00 0.00
-0.00 8.17 0.00
0.00 0.00 8.13
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.26
Polycrystalline dielectric constant εpoly
(total)
8.16
Refractive Index n
2.07
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2CuF4 (mp-760122) 0.2050 0.099 3
Ga3NO3 (mp-754929) 0.1853 0.043 3
Be2GeO4 (mp-768285) 0.1599 0.000 3
Be2SiO4 (mp-3347) 0.0608 0.000 3
Be(PN2)2 (mp-1019545) 0.1350 0.000 3
LiGaGeO4 (mp-8702) 0.3123 0.000 4
LiAlVO4 (mp-770509) 0.2908 0.061 4
LiAlVO4 (mp-770365) 0.3313 0.066 4
LiZnAsO4 (mp-18048) 0.3485 0.000 4
LiAlGeO4 (mp-16947) 0.3304 0.015 4
Cr3N4 (mp-1014558) 0.1074 0.170 2
Ge3N4 (mp-672289) 0.2692 0.000 2
Si3N4 (mp-2245) 0.2644 0.000 2
Ge3N4 (mp-13852) 0.0801 0.002 2
C3N4 (mp-1985) 0.0888 0.322 2
NdAl6Si30(N15O)3 (mp-532626) 0.6635 0.067 5
Li4Al3Ge3IO12 (mp-557456) 0.6016 0.000 5
Li4Al3Ge3BrO12 (mp-554733) 0.6518 0.000 5
YAl6Si30(N15O)3 (mp-686618) 0.6796 0.066 5
YAl6Si30(N15O)3 (mp-677140) 0.6672 0.084 5
C (mp-568410) 0.6455 0.507 1
C (mp-1008374) 0.3317 0.437 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

The commercial PEEK (GATONE, Grade 5300PF) was used as matrix. The silicon nitride (Si3N4) nanoparticles purchased from Aldrich Chemical Company was used as reinforcement. The density and BET specifi [...]
Pressureless sintered -Si3N4 materials containing either 0, 17 or 34 wt% of SiC and 105wt% Al2O3 + 45 wt% Y2O3 additives were heat-treated to stabilize the microstructure by devitrification of the [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition Si3N4.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si N
Final Energy/Atom
-8.1822 eV
Corrected Energy
-117.4382 eV
Uncorrected energy = -114.5502 eV Composition-based energy adjustment (-0.361 eV/atom x 8.0 atoms) = -2.8880 eV Corrected energy = -117.4382 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 74740
  • 187736
  • 644690
  • 79798
  • 644680
  • 100135
  • 35568
  • 170004
  • 170005
  • 170002
  • 35566
  • 98634
  • 170006
  • 23671
  • 34023
  • 35570
  • 98635
  • 170003
  • 16818
  • 170001
  • 35567
  • 35571
  • 35569
  • 8263
Submitted by
User remarks:
  • Silicon nitride - beta

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)