Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.824 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.098 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCsLiF2 + CsF + F2 + NF2 |
Band Gap2.707 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 146.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 219.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 292.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 146.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 206.6 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 253.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 292.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 219.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 146.1 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 219.1 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 206.6 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 206.6 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 292.1 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 103.3 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 126.5 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 73.0 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 103.3 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 126.5 |
C (mp-66) | <1 1 1> | <1 0 0> | 219.1 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 73.0 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 103.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 292.1 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 103.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 73.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 103.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 292.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 219.1 |
Al (mp-134) | <1 1 0> | <1 1 0> | 206.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 292.1 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 73.0 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 73.0 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 103.3 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 103.3 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 146.1 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 1> | 253.0 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 206.6 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 292.1 |
Si (mp-149) | <1 0 0> | <1 0 0> | 146.1 |
Au (mp-81) | <1 0 0> | <1 0 0> | 292.1 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 292.1 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 219.1 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 146.1 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 292.1 |
CdWO4 (mp-19387) | <1 0 0> | <1 1 1> | 126.5 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 73.0 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 292.1 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 292.1 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 219.1 |
ZnO (mp-2133) | <1 1 1> | <1 0 0> | 292.1 |
GaSb (mp-1156) | <1 1 0> | <1 0 0> | 219.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
42 | -18 | -18 | 0 | 0 | 0 |
-18 | 42 | -18 | 0 | 0 | 0 |
-18 | -18 | 42 | 0 | 0 | 0 |
0 | 0 | 0 | 35 | 0 | 0 |
0 | 0 | 0 | 0 | 35 | 0 |
0 | 0 | 0 | 0 | 0 | 35 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
61.6 | 44.7 | 44.7 | -0.0 | -0.0 | -0.0 |
44.7 | 61.6 | 44.7 | -0.0 | -0.0 | 0.0 |
44.7 | 44.7 | 61.6 | -0.0 | -0.0 | 0.0 |
-0.0 | -0.0 | -0.0 | 28.4 | 0.0 | -0.0 |
-0.0 | -0.0 | -0.0 | 0.0 | 28.4 | -0.0 |
-0.0 | 0.0 | 0.0 | -0.0 | -0.0 | 28.4 |
Shear Modulus GV33 GPa |
Bulk Modulus KV2 GPa |
Shear Modulus GR33 GPa |
Bulk Modulus KR2 GPa |
Shear Modulus GVRH33 GPa |
Bulk Modulus KVRH2 GPa |
Elastic Anisotropy0.04 |
Poisson's Ratio-0.75 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cs3CeF6 (mp-632715) | 0.1045 | 0.000 | 3 |
Cs3TbF6 (mp-696965) | 0.0501 | 0.000 | 3 |
Ba3WO6 (mp-25172) | 0.1314 | 0.055 | 3 |
Co(N2Cl)3 (mp-1080142) | 0.0613 | 2.593 | 3 |
CsTlF3 (mp-1078203) | 0.1935 | 0.000 | 3 |
Cs2RbInF6 (mp-989605) | 0.0225 | 0.000 | 4 |
K2SBrCl6 (mp-989587) | 0.0085 | 0.098 | 4 |
Cs2TlInF6 (mp-989537) | 0.0141 | 0.000 | 4 |
KRb2TiF6 (mp-6074) | 0.0222 | 0.000 | 4 |
Cs2KRhF6 (mp-561561) | 0.0244 | 0.000 | 4 |
Ca3Sb2 (mp-1013546) | 0.7358 | 0.379 | 2 |
Ba3Sb2 (mp-1013582) | 0.7358 | 0.415 | 2 |
Fe4N (mp-535) | 0.7358 | 0.288 | 2 |
Ca3Bi2 (mp-1013735) | 0.7358 | 0.366 | 2 |
Sr3Sb2 (mp-1013583) | 0.7358 | 0.379 | 2 |
K2NaNb(OF2)2 (mp-684816) | 0.3387 | 0.087 | 5 |
K2NaVOF5 (mp-690635) | 0.3758 | 0.000 | 5 |
Cs2KZrOF5 (mp-40143) | 0.3644 | 0.000 | 5 |
KRb2ZrOF5 (mp-39542) | 0.3630 | 0.021 | 5 |
Cs2RbZrOF5 (mp-42022) | 0.4022 | 0.007 | 5 |
Ba3LaZnReWO12 (mp-705508) | 0.7246 | 0.061 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Li_sv N F |
Final Energy/Atom-3.8417 eV |
Corrected Energy-38.4167 eV
-38.4167 eV = -38.4167 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)