Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.046 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.022 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSrF2 + CsNaF3 + CsF |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 154.3 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 252.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 154.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 252.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 126.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 126.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 267.3 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 126.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 267.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 252.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 89.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 154.3 |
Al (mp-134) | <1 1 0> | <1 1 0> | 252.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 89.1 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 126.0 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 89.1 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 178.2 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 178.2 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 267.3 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 126.0 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 126.0 |
Si (mp-149) | <1 1 0> | <1 1 0> | 126.0 |
Si (mp-149) | <1 1 1> | <1 1 1> | 154.3 |
ZrO2 (mp-2858) | <1 0 0> | <1 1 0> | 252.0 |
CaCO3 (mp-3953) | <0 0 1> | <1 1 1> | 154.3 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 89.1 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 267.3 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 0> | 267.3 |
CaF2 (mp-2741) | <1 1 1> | <1 1 1> | 154.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 252.0 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 252.0 |
C (mp-66) | <1 1 1> | <1 1 1> | 154.3 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 252.0 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 126.0 |
GaP (mp-2490) | <1 1 1> | <1 1 1> | 154.3 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 89.1 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 267.3 |
YAlO3 (mp-3792) | <0 0 1> | <1 1 0> | 252.0 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 252.0 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 267.3 |
Al2O3 (mp-1143) | <1 0 0> | <1 1 0> | 126.0 |
CaF2 (mp-2741) | <1 1 0> | <1 1 0> | 126.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb2NaSbCl6 (mp-989545) | 0.0005 | 0.000 | 4 |
Cs2LiInBr6 (mp-989405) | 0.0045 | 0.000 | 4 |
Cs2NaPbF6 (mp-989556) | 0.0038 | 0.000 | 4 |
K2NaTlF6 (mp-13798) | 0.0060 | 0.000 | 4 |
Cs2CaSnCl6 (mp-989570) | 0.0021 | 0.003 | 4 |
La2O3 (mp-33032) | 0.0446 | 0.889 | 2 |
Ni4N (mp-20839) | 0.0446 | 2.016 | 2 |
Sr3As2 (mp-1013559) | 0.0446 | 0.370 | 2 |
Ca3P2 (mp-1013547) | 0.0446 | 0.143 | 2 |
Ba3P2 (mp-1013551) | 0.0446 | 0.447 | 2 |
KAgF3 (mp-13819) | 0.0445 | 0.000 | 3 |
KHgF3 (mp-7483) | 0.0446 | 0.000 | 3 |
CsAuCl3 (mp-23026) | 0.0445 | 0.072 | 3 |
BaBiO3 (mp-23438) | 0.0138 | 0.024 | 3 |
FeBiO3 (mp-561388) | 0.0417 | 0.239 | 3 |
SrLaNbZnO6 (mp-41918) | 0.0062 | 0.126 | 5 |
BaLaMgBiO6 (mp-41414) | 0.0160 | 0.069 | 5 |
BaCaLaBiO6 (mp-39886) | 0.0273 | 0.125 | 5 |
BaLaTaZnO6 (mp-42054) | 0.0189 | 0.112 | 5 |
BaLaMgTaO6 (mp-40251) | 0.0003 | 0.079 | 5 |
Ba3LaZnReWO12 (mp-705508) | 0.6716 | 0.059 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points28 |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Na_pv Sr_sv F |
Final Energy/Atom-4.3694 eV |
Corrected Energy-43.6939 eV
-43.6939 eV = -43.6939 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)