Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.197 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.024 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYWN3 |
Band Gap1.499 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinAma2 [40] |
HallA 2 2a |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 249.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 206.0 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 177.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 80.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 103.0 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 144.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 308.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 103.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 226.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 206.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 247.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 350.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 185.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 267.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 144.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 41.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 164.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 144.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 247.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 144.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 61.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 288.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 80.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 329.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 61.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 267.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 161.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 350.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 185.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 161.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 177.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 350.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 329.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 329.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 185.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 221.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 241.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 185.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 206.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 267.7 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 295.4 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 276.9 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 249.3 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 295.4 |
Te2Mo (mp-602) | <1 1 0> | <0 1 1> | 295.4 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 221.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 164.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 82.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 164.8 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 221.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
-0.22694 | 0.18327 | -0.83208 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.41390 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.80785 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.88173 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
7.04 | 0.00 | 0.00 |
0.00 | 7.09 | 0.00 |
0.00 | 0.00 | 8.31 |
Dielectric Tensor εij (total) |
||
---|---|---|
20.99 | 0.00 | 0.00 |
0.00 | 22.40 | 0.00 |
0.00 | 0.00 | 24.03 |
Polycrystalline dielectric constant
εpoly∞
7.48
|
Polycrystalline dielectric constant
εpoly
22.47
|
Refractive Index n2.74 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YWN3 (mp-989645) | 0.5358 | 0.015 | 3 |
LaWN3 (mp-989646) | 0.3337 | 0.016 | 3 |
VCdO3 (mp-566829) | 0.4207 | 0.000 | 3 |
NaVO3 (mp-567447) | 0.3793 | 0.001 | 3 |
LaMoN3 (mp-989534) | 0.3922 | 0.023 | 3 |
LiVO2F (mp-764841) | 0.5207 | 0.049 | 4 |
MgTaBiO5 (mvc-7416) | 0.5658 | 0.079 | 4 |
TaZnBiO5 (mvc-7449) | 0.5577 | 0.117 | 4 |
TiZnBiO5 (mvc-7457) | 0.6040 | 0.077 | 4 |
Ca2SbWO6 (mvc-5995) | 0.5949 | 0.148 | 4 |
Al2O3 (mp-755066) | 0.6924 | 0.089 | 2 |
MnN (mvc-13808) | 0.6498 | 0.366 | 2 |
Bi2O3 (mp-23262) | 0.7424 | 0.000 | 2 |
Bi2O3 (mp-37036) | 0.6299 | 0.092 | 2 |
Ba2Tl2Zn2Sn3O10 (mvc-2762) | 0.6767 | 0.360 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv W_pv N |
Final Energy/Atom-9.8535 eV |
Corrected Energy-100.7015 eV
Uncorrected energy = -98.5355 eV
Composition-based energy adjustment (-0.361 eV/atom x 6.0 atoms) = -2.1660 eV
Corrected energy = -100.7015 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)