Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.591 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.068 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg2S + WS2 + S |
Band Gap0.869 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 289.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 231.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 267.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 189.4 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 267.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 212.5 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 106.3 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 116.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 231.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 173.9 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 284.1 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 284.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 58.0 |
Al (mp-134) | <1 0 0> | <0 1 1> | 212.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 231.9 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 267.1 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 94.7 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 231.9 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 231.9 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 231.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 231.9 |
C (mp-66) | <1 0 0> | <1 0 0> | 189.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 189.4 |
LaF3 (mp-905) | <1 0 0> | <0 1 1> | 106.3 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 289.9 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 284.1 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 173.9 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 189.4 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 189.4 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 284.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 289.9 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 231.9 |
Si (mp-149) | <1 1 0> | <0 0 1> | 173.9 |
Au (mp-81) | <1 1 0> | <0 0 1> | 289.9 |
WS2 (mp-224) | <1 0 0> | <1 0 1> | 222.1 |
C (mp-48) | <1 0 0> | <0 0 1> | 58.0 |
C (mp-48) | <1 0 1> | <1 1 0> | 260.0 |
C (mp-48) | <1 1 0> | <0 0 1> | 231.9 |
C (mp-48) | <1 1 1> | <0 0 1> | 231.9 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 173.9 |
NaCl (mp-22862) | <1 1 1> | <1 0 1> | 111.0 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 231.9 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 116.0 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 116.0 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 267.1 |
SiC (mp-8062) | <1 1 0> | <0 1 0> | 267.1 |
SiC (mp-8062) | <1 1 1> | <1 1 0> | 130.0 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 267.1 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 222.1 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 0> | 89.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiAgF2 (mp-752525) | 0.5529 | 0.093 | 3 |
Ba3(BrO)2 (mp-779533) | 0.5708 | 0.047 | 3 |
Ba3(ClO)2 (mp-756978) | 0.5488 | 0.074 | 3 |
Pb3(IO)2 (mp-619661) | 0.6074 | 0.000 | 3 |
NaVN2 (mp-1029711) | 0.6116 | 0.000 | 3 |
K3LiSiO4 (mp-561474) | 0.6404 | 0.000 | 4 |
TaTl2AgS4 (mp-558241) | 0.5574 | 0.000 | 4 |
K2Li2FeO4 (mp-25751) | 0.5694 | 0.223 | 4 |
BaFe2S2O (mp-1095213) | 0.6192 | 0.000 | 4 |
SrFe2S2O (mp-1095280) | 0.6425 | 0.000 | 4 |
In2Se3 (mp-672673) | 0.7262 | 0.407 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag W_pv S |
Final Energy/Atom-5.2359 eV |
Corrected Energy-157.2202 eV
-157.2202 eV = -146.6048 eV (uncorrected energy) - 10.6154 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)