Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.836 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSc2CoSi2 + ScCoSi |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 273.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 127.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 273.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 156.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 273.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 351.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 117.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 191.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 63.8 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 191.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 117.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 351.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 137.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 78.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 273.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 156.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 156.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 191.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 151.3 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 255.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 273.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 273.6 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 252.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 351.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 127.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 273.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 191.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 302.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 156.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 273.6 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 255.2 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 255.2 |
YVO4 (mp-19133) | <0 0 1> | <0 1 1> | 255.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 127.5 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 252.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 195.4 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 319.1 |
Mg (mp-153) | <1 0 0> | <0 1 1> | 255.2 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 151.3 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 255.2 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 273.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 351.8 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 191.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 117.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 156.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 351.8 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 273.6 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 273.6 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 1 0> | 137.2 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 1 0> | 137.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf3Si3Ni2 (mp-9605) | 0.3883 | 0.000 | 3 |
Y3Si3Pd2 (mp-14244) | 0.4398 | 0.006 | 3 |
Ho3Ge3Ru2 (mp-30172) | 0.1261 | 0.000 | 3 |
Sc3Fe2Si3 (mp-4755) | 0.1431 | 0.000 | 3 |
Sc2Si2Ru (mp-13583) | 0.4430 | 0.008 | 3 |
US2 (mp-669500) | 0.7474 | 0.000 | 2 |
USe2 (mp-20077) | 0.7330 | 0.036 | 2 |
Ca3Ga5 (mp-30473) | 0.6175 | 0.000 | 2 |
Sn3Pd (mp-1371) | 0.7386 | 0.001 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sc_sv Co Si |
Final Energy/Atom-7.0218 eV |
Corrected Energy-111.9230 eV
Uncorrected energy = -112.3490 eV
Composition-based energy adjustment (0.071 eV/atom x 6.0 atoms) = 0.4260 eV
Corrected energy = -111.9230 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)