material

BaMgSi

ID:

mp-9934

DOI:

10.17188/1316995


Tags: Barium magnesium silicide (1/1/1)

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.387 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.67 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 42459 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-2657) <1 1 0> <1 1 0> 0.002 156.4
TiO2 (mp-2657) <1 0 1> <1 0 1> 0.002 128.3
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.004 21.7
GaSe (mp-1943) <0 0 1> <0 0 1> 0.010 238.8
Ni (mp-23) <1 1 1> <1 1 1> 0.018 169.4
TePb (mp-19717) <1 0 0> <0 0 1> 0.018 43.4
PbSe (mp-2201) <1 0 0> <0 0 1> 0.023 195.4
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.026 108.5
LaF3 (mp-905) <1 0 0> <1 0 1> 0.032 213.9
MoSe2 (mp-1634) <1 0 0> <1 0 1> 0.035 256.7
SiC (mp-7631) <0 0 1> <0 0 1> 0.035 173.6
GaSb (mp-1156) <1 0 0> <0 0 1> 0.040 195.4
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.043 195.4
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.052 184.3
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.057 312.8
CdSe (mp-2691) <1 0 0> <0 0 1> 0.058 195.4
CdTe (mp-406) <1 0 0> <0 0 1> 0.059 43.4
Cu (mp-30) <1 1 0> <1 1 0> 0.062 312.8
SiC (mp-8062) <1 0 0> <1 0 1> 0.064 171.1
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.070 151.9
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.070 151.9
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.072 221.2
InSb (mp-20012) <1 0 0> <0 0 1> 0.072 43.4
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.073 184.3
Al (mp-134) <1 1 0> <1 0 0> 0.073 184.3
Bi2Te3 (mp-34202) <0 0 1> <1 0 0> 0.074 221.2
KTaO3 (mp-3614) <1 1 0> <1 0 0> 0.079 184.3
Mg (mp-153) <1 1 1> <1 0 0> 0.080 331.8
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.080 184.3
WS2 (mp-224) <0 0 1> <1 0 0> 0.081 221.2
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.081 221.2
GdScO3 (mp-5690) <1 0 0> <1 0 0> 0.082 184.3
Ag (mp-124) <1 0 0> <1 0 1> 0.083 85.6
CsI (mp-614603) <1 0 0> <1 0 0> 0.089 184.3
ZnO (mp-2133) <1 0 1> <1 1 0> 0.090 156.4
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.090 21.7
C (mp-48) <1 0 0> <1 1 0> 0.090 156.4
CdS (mp-672) <1 0 0> <1 1 0> 0.091 312.8
ZnO (mp-2133) <1 1 1> <1 1 1> 0.093 282.4
GaP (mp-2490) <1 0 0> <1 0 0> 0.094 184.3
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.094 184.3
MgO (mp-1265) <1 1 1> <1 0 0> 0.102 221.2
ZnO (mp-2133) <0 0 1> <0 0 1> 0.104 151.9
DyScO3 (mp-31120) <1 0 0> <1 0 0> 0.105 184.3
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.106 213.9
Mg (mp-153) <0 0 1> <1 0 0> 0.109 221.2
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.109 294.9
NaCl (mp-22862) <1 1 1> <1 0 0> 0.118 110.6
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.119 108.5
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.119 184.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
76 12 22 0 0 0
12 76 22 0 0 0
22 22 48 0 0 0
0 0 0 21 0 0
0 0 0 0 21 0
0 0 0 0 0 36
Compliance Tensor Sij (10-12Pa-1)
15.1 -0.4 -6.8 0 0 0
-0.4 15.1 -6.8 0 0 0
-6.8 -6.8 27.1 0 0 0
0 0 0 48 0 0
0 0 0 0 48 0
0 0 0 0 0 28
Shear Modulus GV
25 GPa
Bulk Modulus KV
35 GPa
Shear Modulus GR
23 GPa
Bulk Modulus KR
34 GPa
Shear Modulus GVRH
24 GPa
Bulk Modulus KVRH
35 GPa
Elastic Anisotropy
0.52
Poisson's Ratio
0.22

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
SrHCl (mp-23860) 0.1797 0.000 3
BaHCl (mp-23861) 0.1884 0.000 3
BaMgGe (mp-754515) 0.0504 0.000 3
CaMnGe (mp-20235) 0.0916 0.090 3
PrMnGe (mp-21271) 0.1504 0.127 3
Na2LiGaAs2 (mp-9722) 0.5034 0.000 4
Na2LiAlP2 (mp-9719) 0.5177 0.000 4
K2NaInAs2 (mp-21510) 0.5386 0.000 4
K2LiInAs2 (mp-505431) 0.3893 0.000 4
K3Na2SnBi3 (mp-568329) 0.5366 0.000 4
YbH2 (mp-864603) 0.7477 0.000 2
CaH2 (mp-23713) 0.7403 0.000 2
SrH2 (mp-23714) 0.7465 0.000 2
SrAl2 (mp-1071777) 0.2424 0.013 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Mg_pv Si
Final Energy/Atom
-3.3681 eV
Corrected Energy
-20.2085 eV
-20.2085 eV = -20.2085 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 42459
  • 191039
Submitted by
User remarks:
  • Barium magnesium silicide (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)